Patents
US 9,006,097 B2#22109005 Most CitedActiveUnited States (USPTO)Utility

Cu pillar bump with electrolytic metal sidewall protection

5Forward Citations (#22109005 Global)
0.5/yrCitation Velocity (#18106879 Global)
1.25Citation PageRank (#30110542 Global)
34Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A method of forming a bump structure includes providing a semiconductor substrate and forming an under-bump-metallurgy (UBM) layer on the semiconductor substrate. The method further includes forming a mask layer on the UBM layer, wherein the mask layer has an opening exposing a portion of the UBM layer. The method further includes forming a copper layer in the opening of the mask layer and removing a portion of the mask layer to form a space between the copper layer and the mask layer. The method further includes performing an electrolytic process to fill the space with a metal layer and removing the mask layer.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 34 · Forward citations: 5.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of forming a bump structure, comprising: providing a semiconductor substrate; forming an under-bump-metallurgy (UBM) layer on a semiconductor substrate; forming a mask layer on the UBM layer, wherein the mask layer has an opening exposing a portion of the UBM layer; forming a copper layer in the opening of the mask layer; removing a portion of the mask layer to form a space between the copper layer and the mask layer; performing an electrolytic process to fill the space with a metal layer; and removing the mask layer.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the metal layer comprises nickel.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein the metal layer comprises gold.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (34)

PatentTitleYearCitations
US 2001012542 A1Solution for forming nickel metal thin film and method of forming nickel metal thin film using the said solution—11
US 2001040290 A1Method for forming bump, semiconductor device and method for making the same, circuit board, and electronic device—189
US 6,627,824 B1Support circuit with a tapered through-hole for a semiconductor chip assembly200352
US 6,681,982 B2Pillar connections for semiconductor chips and method of manufacture200462
US 2004069652 A1Method for producing high purity nickle, high purity nickle, sputtering target comprising high purity nickel, and thin film formed by using said spattering target—17
US 2004166661 A1Method for forming copper bump antioxidation surface—90
US 2005032349 A1Low fabrication cost, fine pitch and high reliability solder bump—31
CN 1,585,114 ASemiconductor package substrate structure with electrically connected pad metal protection layer and manufacturing method thereof—39
US 7,008,867 B2Method for forming copper bump antioxidation surface200667
US 2006094226 A1Bumping process—47
US 2006244140 A1Conductive bump structure of circuit board and method for forming the same—38
US 2007184579 A1Method of fabrication on high coplanarity of copper pillar for flip chip packaging application—25
US 7,276,801 B2Designs and methods for conductive bumps200743
US 2008048320 A1Low fabrication cost, fine pitch and high reliability solder bump—21
US 2008230896 A1Copper die bumps with electromigration cap and plated solder—21
US 7,435,325 B2Method for producing high purity nickle, high purity nickle, sputtering target comprising the high purity nickel, and thin film formed by using said spattering target200844
US 2008296761 A1Cylindrical Bonding Structure and method of manufacture—28
US 7,476,564 B2Flip-chip packaging process using copper pillar as bump structure200939
US 2009102032 A1Electronic Device—26
US 2009206476 A1Conductive structure for a semiconductor integrated circuit—7
US 2009233436 A1Semiconductor Device Having High-Density Interconnect Array with Core Pillars Formed With OSP Coating—69
US 2009289324 A1Mask overhang reduction or elimination after substrate etch—24
US 2010018553 A1Method and apparatus for surface treatment of semiconductor substrates using sequential chemical applications—18
US 2010109159 A1Bumped chip with displacement of gold bumps—68
US 2011049706 A1Front Side Copper Post Joint Structure for Temporary Bond in TSV Application—24

Non-Patent Literature (5)

  • Islam, M. N., et al., "Comparative Study of the Dissolution Kinetics of Electrolytic Ni and Electroless Ni-P by the Molten Sn3.5Ag0.5Cu Solder Alloy", Microelectronics Reliability 242 (2003), pp. 2031-2037.
  • Islam, M. N., et al., “Comparative Study of the Dissolution Kinetics of Electrolytic Ni and Electroless Ni—P by the Molten Sn3.5Ag0.5Cu Solder Alloy”, Microelectronics Reliability 242 (2003), pp. 2031-2037.
  • Office Action dated Jun. 13, 2014 from corresponding No. CN 201010250723.9.
  • Office Action dated May 9, 2013 from corresponding application No. TW 099125872.