US 8,999,511 B2#44855338 Most CitedActiveUnited States (USPTO)Utility

Cubic boron nitride sintered body tool

2Forward Citations (#44855338 Global)
0.2/yrCitation Velocity (#35845815 Global)
0.89Citation PageRank (#48126496 Global)
36Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A cBN sintered body tool has the following feature. In at least one cross sectional surface of the cBN sintered body tool taken along a plane perpendicular to a joining surface having the largest area in joining surfaces between the cBN sintered body and the joining layer, a point C and a point D are assumed to represent points away by ¼ of the length of a line segment connecting a point A and a point B shown in a figure. A value obtained when an area of a region surrounded by a line segment connecting the point C and the point D, the first cBN particle, the second cBN particle, and the binder phase is divided by the length of the line segment connecting the point A and point B to each other is 0.14-0.6 μm.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 36 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A cubic boron nitride sintered body tool in which a cubic boron nitride sintered body is joined to a tool base material via a joining layer, wherein said cubic boron nitride sintered body contains cubic boron nitride particles by not less than 30 volume % and not more than 95 volume % and a binder phase by not less than 5 volume % and not more than 70 volume %, said binder phase is composed of at least one first compound and at least one Al compound, or is composed of at least one second compound, said first compound is a compound composed of at least one element belonging to one of a group IV

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (36)

PatentTitleYearCitations
JP S5978978 AHigh density boron nitride sintered body and manufacture—4
US 5,200,372 AMethod for production of high-pressure phase sintered article of boron nitride for use in cutting tool and sintered article produced by the method199335
DE 4,304,104 A1Hard soldered cutting tool with sintered high hardness piece - is hard soldered on shaft groove with L=shaped cross=section, curved and inclined portions—10
JP H06206105 ADiamond coated tool and manufacture thereof—3
JP H0718415 ACutting tool made of surface coated cubic boron nitride base ceramics having hard coating layer with superior adhesion—24
JP H07291732 APolycrystalline cubic boron nitride sintered compact and use thereof—4
JP H10158065 ACubic boron nitride sintered compact and its production—13
JP H11188510 AHard sintered body cutting tool—11
JP H11320218 AHard sintered body tool and manufacture thereof—28
US 6,071,841 ACubic boron nitride sintered body and method of preparing the same200017
JP 2000326111 AThrow away tip—24
US 6,155,755 AHard sintered body tool200078
US 6,737,178 B2Coated PCBN cutting tools200455
US 2005143252 A1High-strength, highly thermally conductive sintered compact of cubic boron nitride—19
JP 2005187260 AHigh-strength high-thermal conductivity cubic boron nitride sintered compact—46
WO 2005/066381 A1Cubic boron nitride sintered compact—55
US 7,081,424 B2High-strength, highly thermally conductive sintered compact of cubic boron nitride200613
JP 2006346777 ASurface coated cemented carbide cutting tool having lubricative coating layer exhibiting excellent wear resistance—11
JP 2007021639 ACutting tool made of surface coated cemented carbide having hard coated layer exhibiting excellent chipping resistance in cutting work of hard-to-cut material—3
EP 1,757,388 A1Surface-coated cutware and process for producing the same—8
WO 2007/039955 A1cBN SINTERED BODY FOR HIGH-QUALITY SURFACE ASPECT MACHINING AND CUTTING TOOL OF cBN SINTERED BODY—32
US 2007110607 A1High strength hard alloy and method of preparing the same—33
CN 101,014,435 ASurface-coated cutware and process for producing the same—17
JP 2007276079 AHIGH-HARDNESS MACHINING CUTTING TOOL MADE OF CUBIC BORON NITRIDE GROUP CERAMICS HAVING EXCELLENT BRAZING BONDING STRENGTH, AND Ag ALLOY BRAZING MAERIAL TO BE USED FOR THE SAME—6
US 2008214383 A1Cubic Boron Nitride Sintered Body—20
CN 101,263,236 AHigh-strength superhard alloy and manufacturing method thereof—33
US 2008254282 A1Cbn Sintered Body for High Surface Integrity Machining and Cbn Sintered Body Cutting Tool—27
WO 2009/010934 A2Method for joining sic-diamond—7

Non-Patent Literature (3)

  • Notice of Grounds of Rejection in Japanese Patent Application No. 2010-243953, dated Feb. 4, 2014.
  • Notice of Grounds of Rejection in Japanese Patent Application No. 2010-243953, dated Oct. 29, 2013.
  • Notification of the First Office Action issued in Application No. 201280002309.3 dated Dec. 31, 2014.