Preparation of X zeolite
Abstract
A method is disclosed for preparing crystalline aluminosilicate X zeolite from a reaction mixture containing only sufficient water to produce X zeolite. In one embodiment, the reaction mixture is self-supporting and may be shaped if desired. In the method, the reaction mixture is heated at crystallization conditions and in the absence of an added external liquid phase, so that excess liquid need not be removed from the crystallized product prior to drying the crystals.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 30 · Forward citations: 2.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method for preparing crystalline X zeolite from a reaction mixture, said method comprising: (a) preparing a self-supporting reaction mixture comprising at least one active, non-zeolitic source of silica, at least one active, non-zeolitic source of alumina, and a source of hydroxide in amounts sufficient to produce X zeolite, and sufficient water to produce X zeolite; (b) aging the mixture at a temperature from about 25° C. to about 60° C. for at least 24 hours to form crystals of X zeolite nuclei; and (c) maintaining said reaction mixture at a temperature of up to about 130° C. for a period
- Claim 2Depends on #1
The method of claim 1 wherein the step (a) occurs in the absence of add
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (30)
Non-Patent Literature (3)
- English translation of JP08208393.
- PCT International Preliminary Report on Patentability Written Opinion, International Application No. PCT/US2010/056719 dated Jun. 5, 2012.
- U.S. Appl No. 10/138,061, filed Apr. 30, 2002, abandoned.