Process for producing improved grain refining aluminum—titanium—boron master alloys for aluminum foundry alloys

0Forward Citations (#128168926 Global)
0.0/yrCitation Velocity (#128168926 Global)
0.56Citation PageRank (#128168926 Global)
8Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

A process is provided for producing aluminum-titanium-boron grain refining master alloys containing soluble titanium aluminide and insoluble aluminum boride particles, the process comprising mixing aluminum-boron alloy powder and K 2 TiF 6 salt to obtain a blended mixture, heat treating the mixed powder blend thus obtained in an inert gas furnace just below the melting point of aluminum, at approximately 650 degrees Celcius sufficiently long and compacting the heated powder blend in the form of tablets. The cast grain size of an aluminum- 7 wt % silicon foundry alloy after inoculation with this master alloy at an addition level of 0.02% Ti was less than 200 microns for contact times of upto 15 minutes.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method to produce Al—Ti—B grain refiner master alloys with Al 3 Ti particles and AlB 2 particles dispersed in an aluminium matrix, comprising; a. thoroughly mixing Al—B alloy powder and K 2 TiF 6 salt to obtain a blended mixture, b. heating the mixed powder blend under flowing argon to between 600 Centigrade and 650 Centigrade, c. holding the mixed powder blend at this temperature for ½ hours, d. pressing the heat treated powder blend into pellets.

  2. Claim 2Depends on #1

    A method according to claim 1 , wherein the boron content of the Al—B alloy is between 1 to 10 wt %.

  3. Claim 3Depends on #1

    A method according to claim 1 , wherein the Al—B alloy powder is prepared by a. adding KBF 4 salt into molten aluminium to facilitate a salt reaction to form the AlB 2 particles dispersed in an aluminium matrix, b. pulverizing the alloy

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.