Patents
US 8,992,808 B2#50300374 Most CitedActiveUnited States (USPTO)Utility

Method of manufacturing pre-sintered Si-mixture granule for porous sintered reaction-bonded silicon nitride, porous pre-sintered granule manufactured by the method, and method of manufacturing porous sintered reaction-bonded silicon nitride

1Forward Citations (#50300374 Global)
0.1/yrCitation Velocity (#47356259 Global)
0.86Citation PageRank (#50166451 Global)
6Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to a method of manufacturing a porous pre-sintered granule for a sintered reaction-bonded silicon nitride, to which a pressure forming technology can be applied to obtain a porous sintered reaction-bonded silicon nitride having high porosity and having a structure in which macropores and micropores coexist with each other, and to a porous pre-sintered granule manufactured by the method. The method includes the steps of: granulating a raw material comprising silicon and sintering additives including yttrium, aluminum and at least one alkali earth metal compound; and pre-sintering the granulated raw material at a temperature of 1300˜1375° C. under an inert atmosphere. According to the present invention, a porous pre-sintered granule for porous sintered reaction-bonded silicon nitride, which can increase the air permeability and trapping efficiency by controlling the size of a pore channel such that macropores and micropores coexist, can be manufactured.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 1.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a porous sintered reaction-bonded silicon nitride, comprising the steps of: granulating a raw material comprising silicon and sintering additive including yttrium, aluminum, and at least one alkali earth metal compound; pre-sintering the granulated raw material at a temperature of 1300˜1375° C. under an inert atmosphere to prepare porous granules; forming a compact with the porous granules; nitriding the compact under a nitridation atmosphere; and sintering the nitrided compact at a temperature of 1700˜1900° C. under a nitrogen atmosphere.

  2. Claim 2Depends on #1

    The method of manufacturing a porous sintered reaction-bonded silicon nitride according to claim 1 , wherein the sintering additive is included in the raw material in an amount of 2˜5 wt % based on an amount required for the complete nitridation of silicon

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗