High intrinsic viscosity melt phase polyester polymers with acceptable acetaldehyde generation rates
Abstract
A method for the production of solid polyester polymer particles comprising: a) polycondensing a molten polyester polymer composition in the presence of a polycondensation catalyst composition comprising antimony species; b) continuing the polycondenzation of the molten polyester polymer composition to an It.V. of 0.68 dL/g or more; and c) after reaching an It.V. of 0.68 dL/g or more, adding a catalyst stabilizer or deactivator to the polymer melt; and d) after reaching an It.V. of 0.68 dL/g or more, solidifying the melt into solid polyester polymer particles which do not contain organic acetaldehyde scavengers. In a further embodiment, after solidification of the polyester from the melt phase polycondenzation process: e) the amount of residual acetaldehyde in the particles in the solid state is reduced to a level of 10 ppm or less without increasing the It.V. of the particles by more than 0.03 dL/g. Such particles having an AA (acetaldehyde) generation rate of 20 ppm or less upon being melted after solidification following the melt phase production and a free AA level reduced after melt phase production to 10 ppm or less are introduced into a melt processing zone to make articles
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 3.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
Finished polyester polymer particles obtained by a process comprising polycondensing a molten polyester polymer composition to an It.V. of at least 0.68dL/g; then adding at least one antimony catalyst stabilizer or deactivator comprising an acidic phosphorous compound to the polymer melt; and then solidifying the polymer melt into solid polyester polymer particles, and having: a degree of crystallinity of at least 20%, antimony atoms, phosphorus atoms, an acetaldehyde generation rate of less than 20 ppm, as measured at 295° C. for 5 minutes, lacking organic acetaldehyde scavengers, and which h
- Claim 2Depends on #1
The finished particles of claim 1 , wherein the particles have a residual acetaldehyde level of 10 ppm