Patents
US 8,986,789 B2#43636111 Most CitedActiveUnited States (USPTO)Utility

Stress-reduced Ni-P/Pd stacks for bondable wafer surfaces

2Forward Citations (#43636111 Global)
0.2/yrCitation Velocity (#35793794 Global)
0.93Citation PageRank (#46263047 Global)
26Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The invention relates to a substrate having a bondable metal coating comprising, in this order, on an Al or Cu surface: (a) a Ni—P layer, (b) a Pd layer and, optionally, (c) an Au layer, wherein the thickness of the Ni—P layer (a) is 0.2 to 10 m, the thickness of the Pd layer (b) is 0.05 to 1.0 m and the thickness of the optional Au layer (c) is 0.01 to 0.5 m, and wherein the Ni—P layer (a) has a P content of 10.5 to 14 wt.-%. The deposit internal stress of the resulting Ni—P/Pd stack is not higher than 34.48M−Pa (5,000 psi). Further, a process for the preparation of such a substrate is described.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for the preparation of a substrate having a bondable metallic coating comprising, in this order, on an Al or Cu surface: (a) a Ni—P layer having a thickness of 0.2 to 10 μm and a P content of 10.5 to 14 wt.-%, (b) a Pd layer having a thickness of 0.05 to 1.0 μm and, optionally, (c) an Au layer having a thickness of 0.01 to 0.5 μm, wherein a stack consisting of a Ni—P layer (a) and a Pd layer (b) has a deposit internal stress not higher than 34.48 MPa (5,000 psi), the process comprising the following steps: (i) immersing a substrate having an Al or Cu surface in a Ni—P plating bath co

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (26)

PatentTitleYearCitations
US 3,685,582 AElectroless metal plating techniques for consolidation of incompetent formations197210
US 3,969,554 APrecious metal sensitizing solutions197626
US 4,125,648 AElectroless deposition of nickel on aluminum197827
US 4,169,171 ABright electroless plating process and plated articles produced thereby197945
US 4,424,241 AElectroless palladium process198479
WO 9,426,954 A1Palladium layers deposition process—7
DE 4,415,211 A1Verfahren zur Abscheidung von Palladiumschichten—11
EP 0,698,130 A1Palladium layers deposition process—4
EP 0,701,281 A2Substrate with bondable layer—16
US 6,150,186 AMethod of making a product with improved material properties by moderate heat-treatment of a metal incorporating a dilute additive200065
EP 1,126,519 A2Structure and method for bond pads of copper-metallized intergrated circuits—9
JP 2001358164 AElectrode formed with electroless multilayer plating film thereon, and its manufacturing method—16
JP 2002203925 AExternal connection terminal and semiconductor device—52
US 6,445,069 B1Electroless Ni/Pd/Au metallization structure for copper interconnect substrate and method therefor200261
US 2002121709 A1External connection terminal and semiconductor device—65
JP 2004200644 AWiring board—19
US 6,800,121 B2Electroless nickel plating solutions200431
US 2005048309 A1Metal member coated with metal layers—15
JP 2005068445 AMetallic member covered with metal—8
JP 2005072282 AWiring board—10
JP 2005183462 AWiring board—6
WO 2006/040847 A1Printed wiring board and method for manufacturing printed wiring board—3
US 2006086619 A1Method of forming conductive pattern, wiring substrate, electronic device and electronic equipment—14
JP 2006128228 AForming method of conductive film, wiring board, electronic device, and electronic equipment—12
JP 2007258647 ASemiconductor light emitting device, and semiconductor light emitting element—27
US 2008264681 A1Printed Wiring Board and Method for Manufacturing Printed Wiring Board—50

Non-Patent Literature (4)

  • B. Lonyuk et al., "Effect of high-phosphorus electroless nickel coating on fatigue life of Al-Cu-Mg-Fe-Ni alloy", Scripta Materialia, vol. 57, pp. 783-786 (2007).
  • B. Lonyuk et al., "Effect of high-phosphorus electroless nickel coating on fatigue life of Al—Cu—Mg—Fe—Ni alloy", Scripta Materialia, vol. 57, pp. 783-786 (2007).
  • G.O. Mallory et al., "Electroless Plating: Fundamentals and Applications", American Electroplaters and Surface Finishers Society (1989).
  • W. Riedel et al., "Electroless Nickel Plating", Finishing Publications Ltd., 1991.