US 8,986,779 B2#34103356 Most CitedActiveUnited States (USPTO)Utility

Methods of improving surface roughness of an environmental barrier coating and components comprising environmental barrier coatings having improved surface roughness

3Forward Citations (#34103356 Global)
0.3/yrCitation Velocity (#27855812 Global)
0.94Citation PageRank (#45290477 Global)
44Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Methods for improving surface roughness of an environmental barrier coating. The methods include providing a component having a plasma sprayed environmental barrier coating, applying an outer layer repair slurry to the environmental barrier coating of the component, drying the environmental barrier coating having the applied outer layer repair slurry, and sintering the component to produce a component having an improved surface roughness. The outer layer repair slurry includes water, a primary outer material of BSAS, and a slurry sintering aid selected from rare earth nitrate, rare earth acetate, rare earth chloride, rare earth oxide, ammonium phosphate, phosphoric acid, polyvinyl phosphonic acid, and combinations thereof.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 44 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for reducing a surface roughness of an environmental barrier coating, the method comprising: providing a component having a plasma sprayed environmental barrier coating having a surface characterized by a surface roughness; applying an outer layer repair slurry to the surface of the environmental barrier coating of the component; drying the applied outer layer repair slurry; and sintering the applied outer layer repair slurry to form a sintered outer repair layer that defines an outer surface having a lower surface roughness than the surface of the environmental barrier coating; where

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (44)

PatentTitleYearCitations
JP S6067601 APreparation of sintered body—11
US 4,935,390 AMullite-based ceramic body199025
US 5,294,576 AMullite ceramic compound199426
JP H09295872 ACoating agent for sintering jig—10
US 5,759,932 ACoating composition for metal-based substrates, and related processes199859
JP H10183013 ACoating composition for metal base, and related process—6
US 5,985,368 ACoating composition for metal-based substrates, and related processes199987
US 6,159,553 AThermal barrier coating for silicon nitride200059
US 6,294,261 B1Method for smoothing the surface of a protective coating2001112
JP 2002173783 AMethod for applying high-temperature bond coat on metal substrate, and delayed composition and article—12
US 6,410,148 B1Silicon based substrate with environmental/ thermal barrier layer2002118
US 6,497,758 B1Method for applying a high-temperature bond coat on a metal substrate, and related compositions and articles200227
US 2003118440 A1Smart coating system with chemical taggants for coating condition assessment—47
US 6,617,037 B2Silicon based substrate with a CTE compatible layer on the substrate200343
US 6,677,064 B1In-situ formation of multiphase deposited thermal barrier coatings200436
US 2004028941 A1Protective overlayer for ceramics—47
US 6,787,195 B2Method of depositing a coating on Si-based ceramic composites200461
US 6,797,327 B1System and method for forming a low temperature cured ceramic coating for elevated temperature applications20047
JP 2004277237 ASilicon nitride ceramic having steam corrosion resistant layer at high temperature—6
US 2005025983 A1System and method for forming a low temperature cured ceramic coating for elevated temperature applications—10
JP 2005200226 AEnvironmentally resistant film material, film structure and ceramic structure using the same—16
US 6,933,061 B2Thermal barrier coating protected by thermally glazed layer and method for preparing same200539
JP 2006052466 AProcess for deposition of protective coating and article to be coated—23
US 2006121295 A1Sintering resistant, low conductivity, high stability thermal barrier coating/environmental barrier coating/environmental barrier coating system for a ceramic-matrix composite (CMC) article to improve high temperature capability—35
US 7,138,183 B2Environmental barrier coating material and coating structure and ceramic structure using the same200622
US 2006280963 A1Thermal/environmental barrier coating system for silicon-containing materials—52
US 2006280954 A1Corrosion resistant sealant for outer EBL of silicon-containing substrate and processes for preparing same—82

Non-Patent Literature (5)

  • Non-Final Rejection towards corresponding U.S. Appl. No. 12/627,558 dated Jul. 29, 2014.
  • Unofficial English translation of Office Action issued in connection with corresponding JP Application No. 2010-168729 on Jul. 29, 2014.
  • Unofficial English translation of Office Action issued in connection with corresponding JP Application No. 2010-168744 on Sep. 16, 2014.
  • Unofficial English translation of Office Action issued in connection with corresponding JP Application No. 2010-169923 on Sep. 16, 2014.
  • Unofficial English translation of Office Action issued in connection with corresponding JP Application No. 2010-169924 on Sep. 16, 2014.