Method of preparing porous carbonate apatite from natural bone
Abstract
A method for preparing carbonate apatite from natural bones. The method includes obtaining cancellous bone particles; treating the bone particles with hot water and an organic solvent; repeating the treating step at least once; drying the bone particles; and heating the bone particles at 500° C. to 620° C. for 10 to 50 hours.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 3.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of preparing carbonate apatite from natural bone, the method consisting of: providing cancellous bone particles; treating the bone particles with hot water and an organic alcohol to remove lipids therefrom; repeating the treating step at least once; drying the treated bone particles; and heating the dried treated bone particles at 500° C. to 620° C. for 10 to 50 hours.
- Claim 2Depends on #1
The method of claim 1 , wherein the size of the bone particles is 2 mm to 15 mm.
- Claim 3Depends on #2
The method of claim 2 , wherein the size of the bone particles is 5 mm to 10 mm.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (5)
Non-Patent Literature (1)
- Murugan et al., Trends Biomater. Artif. Organs, vol. 20(1), pp. 35-39, 2006.