US 8,975,198 B2#31981144 Most CitedActiveUnited States (USPTO)Utility

Glass with improved pitch stability

3Forward Citations (#31981144 Global)
0.3/yrCitation Velocity (#27731127 Global)
1.12Citation PageRank (#35503487 Global)
12Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Described herein are alkali-free, boroalumino silicate glasses exhibiting desirable physical and chemical properties for use as substrates in flat panel display devices, such as, active matrix liquid crystal displays (AMLCDs) and active matrix organic light emitting diode displays (AMOLEDs). In accordance with certain of its aspects, the glasses possess excellent compaction and stress relaxation properties.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 3.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A glass exhibiting the following performance criteria: A: Compaction in the LTTC less than or equal to 5.5 ppm B: Compaction in the HTTC less than or equal to 40 ppm C: Less than 50% of an induced stress relaxed in the SRTC, wherein the glass comprises, on an oxide basis, between 2.5 and 4.5 mole percent of B 2 O 3 .

  2. Claim 2Depends on #1

    The glass of claim 1 comprising, in mole percent on an oxide basis: SiO 2 50-85, Al 2 O 3 0-20, MgO 0-20, CaO 0-20, SrO 0-20, BaO 0-20, where SiO 2 , Al 2 O 3 , MgO, CaO, SrO and BaO represent the mole percents of the oxide components.

  3. Claim 3Depends on #1

    The glass of claim 1 comprising, in mole percent on an oxide basis: SiO 2 68-74, Al 2 O 3 10-13, MgO 0-6, CaO 4-9, SrO 1-8, BaO 0-5, where SiO 2 , Al 2 O 3 , MgO, CaO, SrO and BaO represent the mole percents of the oxide components.