Provided are resin-based and metal-based anti-thermally-expansive members each having small thermal expansion. More specifically, provided are an anti-thermally-expansive resin and an anti-thermally-expansive metal, each including a resin or a metal having a positive linear expansion coefficient at 20° C. and a solid particle dispersed in the resin or metal, in which the solid particle includes at least an oxide represented by the following general formula (1): (Bi 1-x M x )NiO 3 (1), where M represents at least one metal selected from the group consisting of La, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, Lu, Y, and In; and x represents a numerical value of 0.02≦x≦0.15.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 1.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A metal composite, comprising: a metal having a positive linear expansion coefficient at 20° C.; and a solid particle, which has negative thermal expansion properties at a normal condition and which is dispersed in the metal, wherein the solid particle comprises at least an oxide represented by general formula (1): (Bi 1-x M x )NiO 3   (1), where M represents at least one metal selected from the group consisting of La, Pr, Nd, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, Lu, Y, and In; and x represents a numerical value of 0.02≦x≦0.15.

  2. Claim 2Depends on #1

    The metal composite according to claim 1 , wherein a linear expansion coefficient α at 20° C. of the metal having a positive linear expansion coefficient is 10×10 −6 /K or more and 30×10 −6 /K or less.

  3. Claim 3Depends on #2

    The metal composite according to claim 2 , wherein the metal havi

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (21)

PatentTitleYearCitations
JP S61175035 AComposite body of resin and inorganic material—16
US 4,999,336 ADispersion strengthened metal composites199165
US 5,694,503 AArticle comprising a temperature compensated optical fiber refractive index grating1997134
JP H1096827 AArticle having optical fiber including refractive index grating—19
US 6,132,676 AMinimal thermal expansion, high thermal conductivity metal-ceramic matrix composite200026
US 2002175403 A1Thermal interface material and heat sink configuration—66
US 2003062553 A1Epitaxial template and barrier for the integration of functional thin film metal oxide heterostructures on silicon—64
CN 1,526,029 AThermal interface material and heat sink configuration—20
US 2005191515 A1Very low thermal expansion composite—22
US 2005223846 A1Isotropic zero CTE reinforced composite materials—6
WO 2006/011590 A1Thermal expansion suppressing agent, zero thermal expansion material, negative thermal expansion material, method for suppressing thermal expansion, and method for producing thermal expansion suppressing agent—22
US 2006118160 A1Thermoelectric element and thermoelectric module—50
US 7,187,083 B2Thermal interface material and solder preforms200714
US 2007125412 A1Conductive paste for connecting thermoelectric conversion material—20
US 2007135550 A1Negative thermal expansion material filler for low CTE composites—22
JP 2008260892 AAdhesive agent for electronic parts—13
US 2009004087 A1Thermal Expansion Inhibitor, Zero Thermal Expansion Material, Negative Thermal Expansion Material, Method for Inhibiting Thermal Expansion, and Method for Producing Thermal Expansion Inhibitor—10
JP 2010021429 AElectronic apparatus, and manufacturing method thereof—11
JP 2010029990 ANegative thermal expansion coefficient material and composite material including the same—14
US 7,663,242 B2Thermal interface material and solder preforms201022
US 2012040196 A1Thermal expansion suppressing member and anti-thermally-expansive member—5

Non-Patent Literature (5)

  • Extended European Search Report in Application No. 11177212.5 (Dec. 2011).
  • Extended European Search Report in European Application No. 11177211.7 (Oct. 17, 2011).
  • Goodfellows (Polybenzimidazole, 2013, 3 pages).
  • H. Wadati et al., "Valence Changes Associated with the Metal-Insulator Transition in Bi1-xLaxNiO3," 72 Phys. Rev. B 155103-1-155103-5 (Oct. 2005).