CMP slurry and a polishing method using the same
Abstract
The present invention relates to a CMP slurry that is able to reduce dishing generation, when it is applied to polishing or planarization of silicon oxide layer, for example, and a polishing method. The CMP slurry includes a polishing abrasive, a linear anionic polymer, a compound including a phosphoric acid group, and water, and the ratio of CMP polishing speed to a silicon oxide layer: CMP polishing speed to a silicon nitride layer is 30:1 to 50:1.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 5.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A chemical mechanical polishing (CMP) slurry, comprising a polishing abrasive, a linear anionic polymer having a weight average molecular weight of 2,000 to 50,000 and including a carboxylic acid, ammonium phosphate ((NH 4 ) 2 HPO 4 ), a compound having a weight average molecular weight of 30 to 500 and including a hydroxyl group or a carboxyl group, and water, wherein the ratio of CMP polishing speed to a silicon oxide layer : CMP polishing speed to a silicon nitride layer is 30:1 to 50:1, wherein the polishing abrasive is included with 0.1 to 10 parts by weight per 100 parts by weight of the
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗