Polyester composition for improved stress crack resistance in polyester articles
Abstract
Polyester compositions for use in injection stretch blow molded articles having intrinsic viscosities in the range from about 0.65 to about 0.78 dl/g, and carboxyl end group concentrations of about 47 mmole/kg or more are provided. Stretch blow molded articles formed from these polyester compositions and methods to produce these articles are also described.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 5.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A polyester composition for use in an injection stretch blow molded article comprising: i) an intrinsic viscosity in the range from about 0.65 to about 0.78 dl/g, and ii) a carboxyl end group concentration of at least about 47 mmole/kg; wherein the intrinsic viscosity and the carboxyl end group concentration of the polyester composition are measured after the article has been injection stretch blow molded; wherein the composition is adapted to provide the injection stretch blow molded article with a CSC time to failure of 180 minutes or more; and wherein the composition comprises no cyclic anh
- Claim 2Depends on #1
The composition of claim 1 wherein said intrinsic viscosity is in the range of about 0.65 to about 0.75 dl/g.
- Claim 3Depends on #1
The composition of claim 1 wherein said intrinsic viscosity is in the range of about 0.65 to a
Technical Overview & Description