Abstract

By using a coating method, which is a method of manufacturing a transparent conductive film, with low-temperature heating lower than 300° C., a transparent conductive film with excellent transparency, conductivity, film strength, and resistance stability and a method of manufacturing this film are provided. In the method of manufacturing a transparent conductive film, a heat energy ray irradiating step is a step of irradiating with the energy rays while heating under an oxygen-containing atmosphere to a heating temperature lower than 300° C. to form the inorganic film, and the plasma processing step is a step of performing the plasma processing on the inorganic film under a non-oxidizing gas atmosphere at a substrate temperature lower than 300° C. to promote mineralization or crystallization of the film, thereby forming a conductive oxide fine-particle layer densely packed with conductive oxide fine particles having a metal oxide as a main component.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 30 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of manufacturing a transparent conductive film to be formed through following steps: coating a substrate with a coating liquid containing an organometallic compound to form a coating film; drying the coating film to form a dried coating film; irradiating the dried coating film with energy rays while heating the dried coating film under an oxygen-containing atmosphere having a dew-point temperature equal to or lower than −10° C. to a heating temperature less than 300° C. thereby removing an organic component contained in the dried coating film by decomposition and/or burning, thereby f

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (30)

PatentTitleYearCitations
JP S5736714 ATomeidenkyokunoseizohoho—9
JP S57138708 AComposition for forming transparent conductive film and method of forming transparent conductive film—6
JP S57212268 APasty composition for forming transparent electrically conductive film and forming method of said film—9
US 4,369,208 AProcess for producing transparent electroconductive film198322
US 4,420,500 AComposition and process for preparing transparent conducting film198333
US 4,450,100 APaste for forming transparent conductive coating film198416
US 4,460,496 APaste for forming a transparent, conductive film19845
JP S6019610 ACarrier device—14
JP S6126679 ALiquid forming electrically conductive transparent coating film—5
JP S6319046 ARegister testing system—6
JP S6325448 AIndoor machine for heat pump type air-conditioning machine—10
JP S63314714 AManufacture of transparent electricity conducting film—5
JP H0220706 AMethod and device for cooling pavement material—10
JP H04255768 ACoating solution for forming transparent electrically conductive film—7
JP H06203658 ACoating solution for stranparent conductive film formation—14
JP H06325637 ATransparent conductive coating film forming application liquid and low reflecting transparent conductive film—9
JP H1160278 AFormation of transparent conductive film—10
JP 2001106567 ASubstrate for forming transparent electrically conductive film and formation method of the same conductive film—13
JP 2001244464 AMethod of manufacturing metal oxide transistor—33
JP 2002076356 ASemiconductor device—3,884
US 2002087018 A1Metal organic precursors for transparent metal oxide thin films and method of making same—15
JP 2003308893 AMethod of forming metal oxide semiconductor film, organic pigment sensitizing metal oxide semiconductor electrode and solar battery having the same—18
US 7,132,373 B2Thin metal oxide film and process for producing the same200619
JP 2007123699 AThin-film transistor and method of manufacturing same—20
JP 2007123698 AThin-film transistor and method of manufacturing same—13
JP 2007123700 AMethod of patterning oxide semiconductor and method of manufacturing thin-film transistor—25
JP 2007201366 AField effect transistor—72

Non-Patent Literature (2)

  • K. Nomura et al.-Nature, 2004, vol. 432, pp. 488-492.
  • K. Nomura et al.—Nature, 2004, vol. 432, pp. 488-492.