Patents
US 8,962,791 B2#27163161 Most CitedActiveUnited States (USPTO)Utility

Polylactic acid stereocomplex compositions and methods for making and using same

4Forward Citations (#27163161 Global)
0.4/yrCitation Velocity (#22218658 Global)
1.09Citation PageRank (#37044507 Global)
12Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Thermoformed PLA stereocomplex parts are made using a PLA stereocomplex composition having a highest crystallization melting temperature from 200 to 215° C. The stereocomplex composition preferably has less than 5 J/g of lower melting (160 to 190° C.) crystallites. The stereocomplex can be pre-annealed in various ways to reduce thermoforming cycle times. The stereocomplex forms parts with low haze and good thermal resistance, at reasonable cycle times.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 4.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process comprising a) forming a mixture of starting PLA resins in which a high D PLA resin constitutes from 25 to 75% by weight of the weight of the PLA resins and a high L PLA resin constitutes from 75 to 25% by weight of the PLA resins, and heating the mixture to a temperature above its highest crystalline melting temperature for a period of from about 5 minutes to 3 hours in the presence of a transesterification catalyst, and then blending the resulting transesterified PLA resins with an additional quantity of a high L PLA resin or high D PLA resin to form a blend provided that the propor

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗