Patents
US 8,962,154 B2#80090685 Most CitedActiveUnited States (USPTO)Utility

Wear resistant inner coating for pipes and pipe fittings

0Forward Citations (#80090685 Global)
0.0/yrCitation Velocity (#80090685 Global)
0.56Citation PageRank (#80090685 Global)
24Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A pipe or pipe fitting for use in harsh environment such as in petroleum refinery processes for cracking petroleum feedstocks, the pipe or pipe fitting comprising a 0.25 to 2.5 mm thick Co-based metallic coating on an internal surface of the pipe body, the coating having a hypereutectic microstructure characterized by carbides in a cobalt matrix and an average carbide grain size of less than 50 microns, and the Co-based metallic composition overlays the pipe internal surface at an interface which is free of heat-affected zone and which has a diffusion zone which is less than 0.002 inches thick.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 24 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A petroleum refinery pipe for use in processes for cracking petroleum feedstocks comprising: a pipe body substrate selected from among carbon steels, alloy steels, and stainless steels; and a Co-based metallic coating on an internal surface of the pipe body wherein the coating has a thickness between about 0.25 and 2.5 mm thick; wherein the coating composition comprises between 31 and 34 wt % Cr, between 16 and 19 wt % Mo, between 2.1 and 2.5 wt % C, between 0.5 and 1.5 wt % Si, up to 1 wt % B, and between 42 and 50 wt % Co; wherein the coating has a hypereutectic microstructure characterized

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (24)

PatentTitleYearCitations
US 3,257,178 ACoated metal article196625
US 3,410,732 ACobalt-base alloys196849
US 3,676,085 ACobalt base coating for the superalloys1972120
US 3,720,537 AProcess of coating an alloy substrate with an alloy197323
US 4,389,439 AErosion resistant tubular apparatus for handling slurries198324
US 4,421,717 AMethod of making wear resistant ferrous based parts198313
US 4,641,864 AWear resistant pipe bend for slurry transport198730
CA 1,235,026 APump liners and a method of cladding the same19882
JP H07300642 ACoating material and metal bath immersion member coated with this material—15
US 5,873,951 ADiffusion coated ethylene furnace tubes199939
US 6,066,191 AHard molybdenum alloy, wear resistant alloy and method for manufacturing the same200024
US 6,117,493 ABearing with improved wear resistance and method for making same200016
US 6,187,147 B1Delayed coker unit furnace200115
US 6,413,582 B1Method for forming metallic-based coating200221
US 2003017358 A1Metal-zirconia composite coating with resistance to molten metals and high temperature corrosive gases—7
US 6,537,388 B1Surface alloy system conversion for high temperature applications200344
US 6,582,126 B2Bearing surface with improved wear resistance and method for making same200312
US 2004001966 A1Corrosion-resistant coatings for steel tubes—40
US 6,749,894 B2Corrosion-resistant coatings for steel tubes200436
US 2005152805 A1Method for forming a wear-resistant hard-face contact area on a workpiece, such as a gas turbine engine part—15
US 2006134455 A1Imparting high-temperature degradation resistance to components for internal combustion engine systems—26
US 7,615,144 B2Hydrocarbon thermal cracking using hardfaced fittings20094
WO 2009/146381 A1Slurry-based manufacture of thin wall metal components—7
JP 2010261056 APropeller for ship—4

Non-Patent Literature (5)

  • Abstract of JP7300642; Nov. 14, 1995.
  • Davis, "Nickel, Cobalt, and Their Alloys", Dec. 2000, ASM Int'l, pp. 362-364.
  • European Search Report, European Application No. 12004537.2, dated Oct. 19, 2012, 4 pages.
  • Kennametal Stellite, "Stellite 1", <http://stellite.com/ProductsServices/HardfacingAlloys/CoredWeldingWire/TubularWire/Stellite1/tabid/152/Default.aspx>, accessed Jul. 12, 2014.
  • Radkevych et al. ("Damage to the Metal of Industrial Pipelines in a Hydrogen Sulfide Environment" Mats. Sci. vol. 39, No. 4, 2003).