Process for production of adhesive optical film
Abstract
A method for production of an adhesive optical film comprises the step of forming an anchor layer by applying an anchor layer-forming coating liquid to the optical film to form a coating with a thickness of 20 μm or less before drying, wherein the anchor layer-forming coating liquid contains a mixed solvent composed mainly of water and an alcohol, and a binder resin, and by drying the coating under drying conditions satisfying both of the following requirements: (1) the drying temperature T is between 40° C. and 70° C.; and (2) the value (T×H) obtained by multiplying the drying temperature T (° C.) by the drying time H (seconds) satisfies the relation 400≦( T×H )≦4,000 to remove the mixed solvent.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for production of an adhesive optical film comprising an optical film, an anchor layer, and a pressure-sensitive adhesive layer placed on at least one side of the optical film with the anchor layer interposed therebetween, the method comprising the step of forming an anchor layer by applying an anchor layer-forming coating liquid to the optical film to form a coating with a thickness of 2 to 17 μm before drying, wherein the anchor layer-forming coating liquid contains a mixed solvent in which total content of water and an alcohol is 99% by weight or more, and a binder resin, and by dr
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (9)
Non-Patent Literature (4)
- Chinese Office Action dated Jan. 13, 2014, issued in corresponding Chinese Application No. 201180039115.6 with English Translation. (14 pages).
- Chinese Office Action dated Jul. 23, 2013, issued in corresponding Chinese Patent Application No. 201180039115.6, w/English translation.
- International Search Report for PCT/JP2011/078774, mailing date of Mar. 13, 2012.
- Notification of Transmittal of Copies of Translation of the International Preliminary Report on Patentabililty (Form PCT/IB/338) of International Application No. PCT/JP2011/078774 mailed Jul. 11, 2013 with Forms PCT/IB/373 and PCT/ISA/237.