hottub.patents
US 8,961,867 B2#53930453 Most CitedActiveUnited States (USPTO)Utility

Dynamic dehydriding of refractory metal powders

1Forward Citations (#53930453 Global)
0.1/yrCitation Velocity (#47495211 Global)
0.82Citation PageRank (#53930453 Global)
50Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Refractory metal powders are dehydrided in a device which includes a preheat chamber for retaining the metal powder fully heated in a hot zone to allow diffusion of hydrogen out of the powder. The powder is cooled in a cooling chamber for a residence time sufficiently short to prevent re-absorption of the hydrogen by the powder. The powder is consolidated by impact on a substrate at the exit of the cooling chamber to build a deposit in solid dense form on the substrate.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 1.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for dehydriding, the method comprising: delivering a metal hydride powder to a converging-diverging nozzle; heating the metal hydride powder, within the converging-diverging nozzle, thereby converting the metal hydride powder to a dehydrided metal powder within the converging-diverging nozzle, wherein the dehydrided metal powder has a hydrogen content of 900 ppm or less; cooling the dehydrided metal powder within the converging-diverging nozzle for a sufficiently small cooling time to prevent reabsorption of hydrogen into the metal powder; and thereafter, depositing the dehydrided met

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the dehydrided metal powder is deposited on the substrate from a distance of less than approximately 10 mm.

  3. Claim 3Independent Claim

    The method of

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 3,436,299 APolymer bonding196929
US 3,990,784 ACoated architectural glass system and method1976222
US 4,011,981 AProcess for bonding titanium, tantalum, and alloys thereof197756
US 4,050,133 AMethod of refurbishing turbine vanes and the like197756
US 4,059,442 AMethod for making a porous tantalum pellet197738
US 4,073,427 ALined equipment with triclad wall construction197888
US 4,135,286 ASputtering target fabrication method197960
US 4,140,172 ALiners and tube supports for industrial and chemical process equipment197947
US 4,141,127 AMethod of refurbishing turbine vane or blade components197959
JP S5467198 AAnti-corrosion material for high temperature weak oxidation atmosphere—9
US 4,202,932 AMagnetic recording medium198052
US 4,209,375 ASputter target198077
US 4,291,104 ABrazed corrosion resistant lined equipment198161
US 4,349,954 AMechanical bonding of metal method198236
EP 0,074,803 A1Clad metal joint closure—29
GB 2,121,441 AProcess for upgrading metal powder—21
US 4,425,483 AEcho cancellation using transversal filters198436
JP S5920470 ATarget for sputtering—20
US 4,435,483 ALoose sintering of spherical ferritic-austenitic stainless steel powder and porous body198429
US 4,459,062 AClad metal joint closure198477
US 4,483,819 AProduction of highly capacitive agglomerated valve metal powder and valve metal electrodes for the production of electrolytic capacitors1984155
US 4,508,563 AReducing the oxygen content of tantalum198574
US 4,510,171 AClad metal joint closure198554
US 4,537,641 AProcess for producing valve-metal anodes for electrolytic capacitors198577
JP S62230967 AMethod for generating used target—18
US 4,722,756 AMethod for deoxidizing tantalum material1988179
JP S6335769 ATarget for sputtering—13
US 4,731,111 AHydrometallurical process for producing finely divided spherical refractory metal based powders1988124
JP S63100177 ATarget for sputtering—14