Method of manufacturing monocrystal, flow straightening cylinder, and monocrystal pulling-up device
Abstract
For manufacturing a monocrystal, a monocrystal pulling-up device controls pressure within a flow straightening cylinder to be from 33331 Pa to 79993 Pa and a flow velocity of inert gas in the cylinder to be from 0.06 m/sec to 0.31 m/sec (0.005 to 0.056 SL/min·cm 2 ) during a post-addition-pre-growth period. By controlling the flow velocity of the inert gas to be in the above-described range during the post-addition-pre-growth period, the inert gas flows smoothly even when the pressure within the cylinder is relatively high. Evaporation of a volatile dopant because of a reverse flow of the inert gas can be restrained. The volatile dopant can be prevented from adhering to the flow straightening cylinder in an amorphous state, and the volatile dopant can be prevented from dropping into a melt or sticking on the melt while growing a crystal. Foulings can be easily removed.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 1.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of manufacturing a monocrystal, comprising: providing a monocrystal pulling-up device comprising: (i) a chamber, (ii) an intake provided on an upper portion of the chamber for introducing an inert gas into the chamber, (iii) a crucible disposed within the chamber for accommodating a dopant-added melt prepared by adding a volatile dopant to a silicon melt, (iv) a flow straightening cylinder extending from the intake of the chamber to a vicinity of a surface of the dopant-added melt for guiding the inert gas to the dopant-added melt, the flow straightening cylinder comprising a first cy
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 11,047,065 B2 | Method for producing silicon single crystal, heat shield, and single crystal pulling device | 2021 | 1 |
References Cited — Backward Prior Art (11)
Non-Patent Literature (2)
- English Language International Search Report dated Aug. 19, 2008, issued in parent Appln. No. PCT/JP2008/063398.
- International Preliminary Report on Patentability (IPRP) dated Mar. 8, 2011 (in English) in parent International Application No. PCT/JP2008/063398.