Abstract
A heating process makes a temperature of joining surfaces Wa and Ta of a pair of metal parts W and T at the start of a first joining process equal to 20% or greater, preferably, 40% or greater of a melting point of material of the metal parts W and T. The heating process makes a heating depth h of the pair of metal parts W and T at the start of the first joining process equal to 1.0 mm or greater.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 43 · Forward citations: 3.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A friction joining method of connecting joining surfaces of a pair of metal parts to each other with the use of frictional heat generated at the joining surfaces of the pair of metal parts, comprising: a heating process heating at least one of the joining surfaces of the pair of metal parts; a contact process, after the completion of the heating process with the joining surfaces of the pair of metal parts being faced to each other, relatively moving one of the metal parts toward the other to bring the joining surfaces of the pair of metal parts into contact with each other; and a joining proce
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (43)
Non-Patent Literature (4)
- International Search Report issued on Jul. 31, 2012 for PCT/JP2012/060929 filed on Apr. 24, 2012 with English Translation.
- International Written Opinion issued on Jul. 31, 2012 for PCT/JP2012/060929 filed on Apr. 24, 2012.
- Machine translation of JP-05-123876A (no date available).
- Machine translation of JP-05-131280A (no date available).