A method for fabricating fine reduced iron powders comprises the following steps: heating fine iron oxide powders having a mean particle size of smaller than 20 μm to a reduction temperature of over 700° C. to reduce the fine iron oxide powder into iron powders that are partially sintered into iron powder agglomerates; and performing a crushing-spheroidizing process on the iron powder agglomerates to obtain individual iron powders having a mean particle size of smaller than 20 μm. The method can reduce iron oxide powers into iron powders having a rounded shape and a high packing density and a high tap density, which are suitable for the metal injection molding process and the inductor fabrication process. The reduced iron powder may further be processed using an annealing process and a second crushing-spheroidizing process in sequence to further increase the sphericity, packing density, and tap density of the reduced iron powder.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 3.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for fabricating fine reduced iron powder, comprising: heating fine iron oxide powders containing over 98 weight percent iron oxide and having a mean particle size of smaller than 20 μm to a reduction temperature of over 700° C. to reduce the fine iron oxide powders in a reducing atmosphere into iron powders that are partially sintered into iron powder agglomerates; and performing a crushing-spheroidizing process on the iron powder agglomerates to crush the iron powder agglomerates into individual iron particles having a rounded shape and a mean particle of smaller than 20 μm.

  2. Claim 2Depends on #1

    The method for fabricating fine reduced iron powders according to claim 1 , wherein the fine iron oxide powder is selected from a group consisting of millscale, magnetite, and hematite powders.

  3. Claim 3Independent Claim

    The method for fabricatin