Glass strengthening and patterning methods
Abstract
High intensity plasma-arc heat sources, such as a plasma-arc lamp, are used to irradiate glass, glass ceramics and/or ceramic materials to strengthen the glass. The same high intensity plasma-arc heat source may also be used to form a permanent pattern on the glass surface—the pattern being raised above the glass surface and integral with the glass (formed of the same material) by use of, for example, a screen-printed ink composition having been irradiated by the heat source.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 3.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A method comprising: strengthening an untreated glass sample by; providing a soda-lime silicate glass have a first surface comprising a tin side, a second surface comprising an air side and edges; providing a plasma-arc heat source capable of delivering a power density of at least 900 W/cm 2 in less than one second; unidirectionally translating the glass under the plasma-arc heat source at a speed of 8 mm/s; irradiating the first surface of the glass with the plasma-arc heat source at a power density of 900 W/cm 2 ; and quenching the glass following irradiation; thereby increasing an equibiax
- Claim 2Depends on #1
The method of claim 1 further comprising annealing the strengthened glass using the plasma-arc
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (11)
Non-Patent Literature (5)
- "Standard Test Method for Flexural Strength of Advanced Ceramics at Ambient Temperature," ASTM C1161, vol. 15.01, ASTM International, West Conshohocken, Pennsylvania (2008).
- "Standard Test Method for Monotonic Equibiaxial Flexure Strength of Advanced Ceramics at Ambient Temperature," ASTM C1499, vol. 15.01, ASTM International, West Conshohocken, Pennsylvania (2008).
- Akcakaya, R. et al., "Fatigue Behavior of Surface Flaws on Air vs. Tin Side of Soda-Lime-Silica Float Glass"; Paper T4.3 in Glass in the New Millennium: Challenges and Break-Through Technologies, Proceedings of the ICG Annual Meeting 2000 (Amsterdam, The Netherlands), National Committee Netherlands
- Barsom, J. M., "Fracture of Tempered Glass," J. Am. Cer. Soc., vol. 51, No. 2, pp. 75-78 (Feb. 1968).
- Fabes, B. D. et al., "Strengthening of Glass by Sol-Gel Coatings," J. Am. Cer. Soc., vol. 73, No. 4, pp. 978-988 (Apr. 1990).