Glass substrate for flat panel display and method for manufacturing same
Abstract
Provided are: a glass substrate for p-Si TFT flat panel displays that is composed of a glass having high characteristic temperatures in the low-temperature viscosity range, typified by the strain point and glass transition point, having a small heat shrinkage rate, and being capable of avoiding the occurrence of the problem regarding the erosion/wear of a melting tank at the time of melting through direct electrical heating; and a method for manufacturing same. The present glass substrate is composed of a glass comprising 52-78 mass % of SiO 2 , 3-25 mass % of Al 2 O 3 , 3-15 mass % of B 2 O 3 , 3-25 mass % of RO, wherein RO is total amount of MgO, CaO, SrO, and BaO, 0.01-1 mass % of Fe 2 O 3 , and 0-0.3 mass % of Sb 2 O 3 , and substantially not comprising As 2 O 3 , the glass having a mass ratio (SiO 2 +Al 2 O 3 )/B 2 O 3 in a range of 7-30 and a mass ratio (SiO 2 +Al 2 O 3 )/RO equal to or greater than 6. The present method for manufacturing a glass substrate involves: a melting step of obtaining a molten glass by melting, by employing at least direct electrical heating, glass raw materials blended so as to provide the aforementioned glass composition; a forming step of forming
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 3.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of manufacturing a glass substrate for a flat panel display, the method comprising: a melting step of melting, by employing at least direct electrical heating, glass raw materials blended so as to provide a glass comprising: 52-78 mass % of SiO 2 , 3-25 mass % of Al 2 O 3 , 3-15 mass % of B 2 O 3 , 3-25 mass % of RO, wherein RO is total amount of MgO, CaO, SrO, and BaO, 0.01-1 mass % of Fe 2 O 3 , and 0-0.3 mass % of Sb 2 O 3 , and substantially not comprising As 2 O 3 , the glass having a mass ratio (SiO 2 +Al 2 O 3 )/B 2 O 3 in a range of 7-30 and a mass ratio (SiO 2 +Al 2 O 3 )/RO
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (26)
Non-Patent Literature (5)
- Communication dated Apr. 11, 2014, issued by the State Intellectual Property Office of the People's Republic of China in corresponding Application No. 201280002211.8.
- Communication dated Jul. 23, 2014, issued by the Korean Intellectual Property Office in corresponding Application No. 10-2012-7031553.
- Decision of Rejection issued in corresponding Taiwanese Patent Application No. 101123759 dated Oct. 8, 2013.
- Form PCT/ISA/220.
- Form PCT/ISA/237.