Patents
US 8,927,445 B2#44798650 Most CitedActiveUnited States (USPTO)Utility

Sealing agent with low softening temperature useful in the preparation of electronic devices

2Forward Citations (#44798650 Global)
0.2/yrCitation Velocity (#35843427 Global)
0.89Citation PageRank (#48029834 Global)
12Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

The invention includes a composition for sealing agent, generally in the form of glass frit, lead-free, comprising by weight over the total weight of the composition: 30-80% Bi 2 O 3 ; 2-10% ZnO; 2-10% B 2 O 3 ; 0-5% Na 2 O; 1-10% SiO 2 ; 1-8% Al 2 O 3 ; 0-7% BaO; and 0-8% MgO. The composition for sealing agent as defined above can be added with a filler in a quantity up to 20% by weight over the total weight of the resulting mixture. The invention also includes a sealing paste containing the composition for sealing agent, the optional filler, an organic binder and optionally an organic solvent. The invention also includes methods for producing and using the composition for sealing agent and the sealing paste, as well as an electronic device sealed with the sealing paste.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 2.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A lead-free composition, comprising about: 60% Bi 2 O 3 , 5% ZnO, 7% B 2 O 3 , 10% SiO 2 , 7% Al 2 O 3 , 6% BaO, 1% MgO, 2% Na 2 O, 1% Y 2 O 3 , and 1% Nd 2 O 3 , based on the total weight of the composition.

  2. Claim 2Depends on #1

    The composition for sealing agent according to claim 1 , in the form of a glass frit.

  3. Claim 3Depends on #1

    A process to prepare the composition for sealing agent according to claim 1 , which comprises the steps of: a) mixing said Bi 2 O 3 , ZnO, B 2 O 3 SiO 2 Al 2 O 3 , B 2 O, MgO, Na 2 O, Y 2 O 3 and Nd 2 O 3 obtaining a homogeneous mixture; b) bringing said homogeneous mixture to a temperature between 800° C. and 1200° C., for about 45 minutes thus forming a molten glass; c) subjecting said molten glass to rapid cooling in water; d) grinding the material obtained in step c), thus obtaining a powder ha

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • International Preliminary Report on Patentability mailed on Jan. 2, 2013 in International Application No. PCT/IT2010/000394, International Filing Date Sep. 16, 2010. (9 pages).
  • International Search Report mailed on May 5, 2011 in International Application No. PCT/IT2010/000394, International Filing Date Sep. 16, 2010. (5 pages).