US 8,921,885 B2#103374150 Most CitedActiveUnited States (USPTO)Utility

Method for forming ohmic electrode and semiconductor light emitting element

0Forward Citations (#103374150 Global)
0.0/yrCitation Velocity (#103374150 Global)
0.56Citation PageRank (#103374150 Global)
13Prior Art Cited
2Claims (2 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention relates to a method of forming an ohmic electrode in a semiconductor light emitting element, comprising: forming a semiconductor layer having a light emitting structure on a substrate, sequentially laminating a bonding layer, a reflective layer and a protective layer on the semiconductor layer, and forming an ohmic electrode by performing a heat treatment process to form ohmic bonding between the semiconductor layer and the bonding layer and to form an oxide film on at least a portion of the protective layer; and a semiconductor light emitting element using the ohmic electrode. According to the present invention, since a reflective layer is formed of Ag, Al and an alloy thereof with excellent light reflectivity, the light availability is enhanced. Further, since contact resistance between a semiconductor layer and a bonding layer is small, it is easy to apply large current for high power.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 0.

Claims (2 — 2 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A semiconductor light emitting element, comprising: a semiconductor layer having a light emitting structure; and an ohmic electrode comprising a bonding layer, a reflective layer and a protective layer sequentially laminated on the semiconductor layer, wherein ohmic bonding is formed between the bonding layer and the semiconductor layer, and the protective layer comprises an oxide film consisting of MgO x and disposed on at least a portion of the protective layer, wherein the reflective layer consists of Ag, and wherein the bonding layer comprises a Ni oxide film formed on at least a portion

  2. Claim 2Independent Claim

    The semiconductor light emitting element as claimed in 1 , wherein the reflective layer is directly disposed on the bonding layer, and the protective layer is disposed directly on the reflective layer.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (4)

  • Final Office Action issued on Feb. 3, 2012 in U.S. Appl. No. 12/296,356.
  • KP 10-2005-0075076 Translation of.
  • Non-Final Office Action dated Aug. 1, 2011 in U.S. Appl. No. 12/296,356.
  • Notice of Allowance issued for related U.S. Appl. No. 12/296,356, dated May 23, 2012.