Polyurethane urea elastic fiber
Abstract
Disclosed is a polyurethane urea elastic fiber containing 5-40% by weight of a polyurethane compound, wherein the compression deformation starting temperature determined by thermomechanical analysis (TMA) is not less than 150° C. but not more than 180° C. and time for thermal cutting at 180° C. is not less than 30 seconds.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 16 · Forward citations: 1.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
Polyurethane urea elastic fiber to provide fabrics suppressed in occurrence of curls and frays containing 60 wt % or more of a polyurethane urea polymer and 5 wt % to 40 wt % of a polyurethane compound, obtained by reacting a polyester diol or a polyether diol (excluding polyoxyethylene glycol), having a number average molecular weight of 500 to 2500, an isocyanate compound and a low molecular-weight polyol, wherein the polyurethane compound has no endothermic peak between 80° C. and a temperature at which decomposition of the polyurethane compound starts in differential scanning calorimetry (
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| JP 2015224399 A | Polyurethane elastic fiber | — | 2 |
References Cited — Backward Prior Art (16)
Non-Patent Literature (1)
- Office Action dated Mar. 16, 2011 issued in corresponding Korean application.