Patents
US 8,920,705 B2#72156229 Most CitedActiveUnited States (USPTO)Utility

Process for producing a powder of aluminum titanate-based ceramics

0Forward Citations (#72156229 Global)
0.0/yrCitation Velocity (#72156229 Global)
0.56Citation PageRank (#72156229 Global)
23Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The invention is to provide a process of producing the powder of aluminum titanate-based ceramics in which the formation of fine particulate component and coarse particulate component is inhibited, and having a very sharp grain size distribution, efficiently and at good yield. The invention is a process for producing a powder of aluminum titanate-based ceramics, comprising a step of keeping a precursor mixture containing a titanium source powder, an aluminum source powder and a silicon source powder at a temperature range of from 1100° C. to 1350° C. for 3 hours or more, followed by a step of heating the precursor mixture up to 1400° C. or more and thereafter firing, at this temperature, the precursor mixture after the keeping to obtain a fired body of aluminum titanate-based ceramics, and a step of pulverizing and classifying the fired body of aluminum titanate-based ceramics, wherein the step of pulverizing and classifying the fired body of aluminum titanate-based ceramics comprises; a step (A) of pulverizing the fired body of aluminum titanate-based ceramics with the application of an impact and classifying the pulverized ceramics to obtain a powder of aluminum titanate-based ce

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 23 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for producing a powder of aluminum titanate-based ceramics, comprising a step of keeping a precursor mixture containing a titanium source powder, an aluminum source powder and a silicon source powder at a temperature range of from 1100° C. to 1350° C. for 3 hours or more, followed by a step of heating the precursor mixture up to a temperature of 1400° C. or more and thereafter firing, at this temperature, the precursor mixture after the keeping to obtain a fired body of aluminum titanate-based ceramics, and a step of pulverizing and classifying the fired body of aluminum titanate-bas

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (23)

PatentTitleYearCitations
DE 29,794 CNeuerungen an Bohrhaltern und Bohrern. (Abhängig vom Patente Nr. 29046.)—7
US 3,825,653 AProcess for preparing sinterable aluminum titanate powder197421
US 4,746,638 AAlumina-titania composite powder and process for preparing the same198832
JP S63236759 ACeramic material for casting—8
US 5,032,376 AMethod for producing aluminum titanate19916
US 5,055,435 ACeramic materials to be insert-cast199119
US 5,055,434 ASinterable pulverulent raw material based on aluminum titanate, a process for its preparation and the sintered bodies produced therefrom and their use199112
US 5,260,116 ACeramicm port liners199318
JP H1160240 AProduction of aluminum titanate powder and sintered compact of aluminum titanate—22
US 6,197,248 B1Process for preparing aluminum titanate powder and sintered body200121
US 6,403,019 B1Process for preparing sintered body of aluminum titanate200224
WO 2004/039747 A1Method for producing aluminum magnesium titanate sintered product—35
WO 2005/105704 A1Magnesium aluminum titanate crystal structure and method for producing same—72
US 2006009347 A1Method for producing aluminum magnesium titanate sintered product—21
EP 1,741,684 A1Magnesium aluminum titanate crystal structure and method for producing same—7
US 2007224110 A1Magnesium Aluminum Titanate Crystal Structure and Method for Producing Same—29
US 7,294,164 B2Narrow pore size distribution aluminum titanate body and method for making same200753
US 2008125305 A1Aluminum titanate batch compositions and method—22
US 2010216634 A1Method for manufacturing honeycomb structure—17
US 2010264568 A1System and method for forming ceramic precursor material for thin-walled ceramic honeycomb structures—5
US RE42352 EMethod for producing aluminum magnesium titanate sintered product20118
US 2012220445 A1Process for producing aluminum titanate-based fired body, and aluminum titanate-based fired body—8
US 2012225768 A1Method for manufacturing ceramic honeycomb structure and coating material for the ceramic honeycomb structure—6

Non-Patent Literature (3)

  • European Search Report issued Apr. 5, 2013 in corresponding European Patent Application No. 09819182.8 to Sumitomo Chemical Co., Ltd.
  • First Office Action issued Dec. 3, 2012 in Chinese Patent Application No. 200980139744.9 to Sumitomo Chemical Co., Ltd., with translation.
  • Sturevant, Inc. NSP Powderizer. Hanover, MA: 1999.