Abstract

A method for producing a clinker substitute for use in cement production includes predrying clay with an iron content >1.5 wt-% in a form of iron oxides and a kaolinite content <40 wt-% to a moisture <10 wt-%. The clay is comminuted to a grain size <2 mm. The clay is calcined by thermal treatment in a furnace at a temperature of 600 to 1000° C. The clay is thermally treated under reducing conditions at a temperature of 600 to 1000° C. so as to form a reduction product. The reduction product is intermediately cooled to a temperature <300° C. and finally cooled.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 17 · Forward citations: 8.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for producing a clinker substitute for use in cement production, the method comprising: a) predrying clay with an iron content >1.5 wt-% in a form of iron oxides and a kaolinite content <40 wt-% to a moisture <10 wt-%; b) comminuting the clay to a grain size <2 mm; c) calcining the clay by thermal treatment in a furnace at a temperature of 600 to 1000° C.; d) thermally treating the clay under reducing conditions at a temperature of 600 to 1000° C. so as to form a reduction product; e) intermediately cooling the reduction product to a temperature <300° C.; and f) finally

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein the clay in step a) has a CaO content >0.1 wt-%.

  3. Claim 3Depends on #1

    The method according to claim 1 , wherein the intermediate cooling of

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • "Integrated Pollution Prevention and Control (IPPC)", Reference Document on Best Available Techniques in the Cement and Lime Manufacturing Industries, European Commission, Brussels, Dec. 1, 2011; Gasafi, E., Jeske, U. and T. Reinhardt, Dec. 1, 2006, "Gipsreduktion mit Kohlenstoff-Rahmenbedingungen f
  • A. Buchwald, et al.: "The suitability of thermally activated illite/smectite clay as raw material for geopolymer binders", Applied Clay Science, vol. 46, No. 3, Nov. 1, 2009, pp. 300-304; XP002675980, chapter; 3 & 4 figure 3.
  • Changling He, et al.: "Thermal stability and pozzolanic activity of calcined illite", Applied Clay Science, vol. 9, Feb. 1, 1995, pp. 337-354. XP002675982, chapter: 3 table 1.
  • Changling He, et al.: "Thermal stability and pozzolanic activity of calcined kaolin", Applied Clay Science, vol. 9, No. 3, Sep. 1, 1994, pp. 165-187, XP002675979, chapter: 3.1 & 3.2.
  • Duda, "Cement-Data-Book", International Process Engineering in the Cement Industry, vol. 1, 3rd edition, Dec. 1985, p. 4.