Propylene polymer composition having superior hexane extractables/impact balance
Abstract
Heterophasic polypropylene copolymers having an MFR (2.16 kg, 230° C.) of 15 to 200 g/10 min, determined according to ISO 1133 comprising a propylene homo- or copolymer matrix with an MFR (2.16 kg, 230° C.) of 80 to 500 g/10 min, determined according to ISO 1133 (A) and an ethylene or C 4 -C 10 -alpha-olefin propylene rubber phase (B) dispersed within the matrix, wherein the heterophasic polypropylene resin has a fraction soluble in p-xylene at 25° C. (XCS), having an intrinsic viscosity of 2.85 to 4.00 dl/g, determined according to DIN EN ISO 1628-1 and -3 and being composed of propylene monomer units in an amount of 70 wt % to 90 wt %, with optimum balance of impact resistance and low amount of hexane extractables; a process for their preparation and their use.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 3.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
Process for the preparation of heterophasic polypropylene copolymers comprising the steps of: producing a polypropylene polymer matrix (A) in the presence of a catalyst system in a first slurry reactor and optionally in a second slurry reactor or in a 1 st gas phase reactor (GPR), yielding a first polymerisation product, wherein the catalyst system comprises: i) a Ziegler-Natta procatalyst which contains a trans-esterification product of a lower alcohol and a phthalic ester; (ii) optionally an organometallic cocatalyst; and (iii) an external donor represented by formula (I) or (II) Si(OCH 2 C
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗