Polypropylene composition suitable for extrusion coating
Abstract
Polypropylene composition comprising a polypropylene base resin whereby the polypropylene base resin has a MFR (2.16 kg, 230° C., ISO 1133) of 8 to 24 g/10 min and a LAOS-NLF>2.8 whereby LAOS−NLF=|G′ 1 /G′ 3 | where G′ 1 —first order Fourier Coefficient, G′3—third order Fourier Coefficient.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 21 · Forward citations: 6.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A polypropylene composition comprising a polypropylene base resin wherein the polypropylene base resin has a MFR (2.16 kg, 230° C., ISO 1133) of 8 to 24 g/10 min and a Large Amplitude Oscillatory Shear Non-Linearity Factor (LAOS-NLF)>2.8 wherein LAOS - N L F = G 1 ′
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (21)
Non-Patent Literature (1)
- International Search Report mailed Mar. 17, 2011 for International application No. PCT/EP2011/000255.