Nanopolymetalic reducing agent filler

1Forward Citations (#47154723 Global)
0.1/yrCitation Velocity (#48608510 Global)
1.00Citation PageRank (#41772523 Global)
4Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention provides a nanopolymetallic reducing agent filler comprising 20%-70% iron powder, 10%-30% tourmaline power, 2%-15% copper power, 3%-10% bamboo charcoal powder, 2%-15% kaoline, 2%-15% magnesite powder, 2%-15% pyrolusite powder, and 10%-30% zeolite powder. All percentages described above are by weight. A process of forming the nanopolymetallic reducing agent filler is also provided, including grinding and ball milling raw materials of each component respectively into powder particles of 10 nm-100 μm, which are then mixed uniformly by weight percentage and granulated to form a granular mixture, and sintering the granular mixture at high temperature or cold pressing it into a granular filler.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A nanopolymetallic reducing agent filler, comprising components that include 20%-40% iron powder, 10%-30% tourmaline power, 2%-15% copper powder, 3%-10% bamboo charcoal powder, 2%-15% kaoline, 2%-15% magnesite powder, 2%-15% pyrolusite powder, and 10%-30% zeolite powder, all percentages described above are by weight.