Patents
US 8,883,258 B2#113390825 Most CitedActiveUnited States (USPTO)Utility

Protective coating of silver

0Forward Citations (#113390825 Global)
0.0/yrCitation Velocity (#113390825 Global)
0.56Citation PageRank (#113390825 Global)
12Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

In the method, silver is protected against tarnishing using an Atomic Layer Deposition method. In the Atomic Layer Deposition method, a thin film coating is formed 5 on the surface of silver by depositing successive molecule layers of the coating material. For example aluminum oxide (Al 2O3) or zirconium oxide may be used as the coating material.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method for protecting silver products, articles or parts against tarnish in an atmosphere, the method consisting of applying a thin coating layer of protective material having a thickness between 60 nm to 90 nm on at least a part of an outer surface of a silver product, article or part using an ALD (Atomic Layer Deposition) method to prevent tarnishing of the outer surface of the silver product, article or part in the atmosphere.

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein applying the thin coating layer comprises providing at least one layer of metal oxide using the ALD (Atomic Layer Deposition) method.

  3. Claim 3Depends on #2

    The method according to claim 2 , wherein the metal oxides comprise aluminum oxide Al 2 O 3 , titanium oxide TiO 2 , chromium oxide Cr 2 O 3 , zirconium oxide ZrO 2 , indium oxide In 2 O 3 , and ni

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (5)

  • Aug. 23, 2012, Office Action cited in JP 2008-552836 (with English translation).
  • Dicing Tape 1008 R: Silikonfrei, Laborprotokoll Reinigung and Beschichtung, Oct. 21, 2009, Selte 10 von 12.
  • Groner et al., "Electrical characterization of thin Al2O3 films grown by atomic layer deposition on silicon and various metal Substrates," Thin Solid Films, vol. 413, pp. 186-197, 2002.
  • Groner, M.D. et al., "Electrical characterization of thin Al2O3 films grown by atomic layer deposition on silicon and various metal substrates," Thin Solid Films, 413 (2002) pp. 186-197.