Patents
US 8,876,989 B2#58284610 Most CitedActiveUnited States (USPTO)Utility

Low rhenium nickel base superalloy compositions and superalloy articles

1Forward Citations (#58284610 Global)
0.1/yrCitation Velocity (#49443803 Global)
0.78Citation PageRank (#58284610 Global)
27Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Low rhenium nickel base superalloy compositions and articles formed from the superalloy composition are provided. The nickel base superalloy composition includes in percentages by weight: about 5-8 Cr; about 6.5-9 Co; about 1.3-2.5 Mo; about 4.8-6.8 W; about 6.0-7.0 Ta; if present, up to about 0.5 Ti; about 6.0-6.4 Al; about 1-2.3 Re; if present, up to about 0.6 Hf; if present, up to 1.5 C; if present, up to about 0.015 B; the balance being nickel and incidental impurities. Exemplary compositions are characterized by an Re ratio defined as the weight % of Re relative to the total of the weight % of W and the wt % of Mo, of less than about 0.3. Exemplary articles include airfoils for gas turbine engine blades or vanes, nozzles, shrouds, and splash plates.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 27 · Forward citations: 1.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A nickel base superalloy composition consisting of, in percentages by weight: 5-8 Cr; 6.5-9 Co; 1.5-2.0 Mo; 6.0-6.5 W; 6.0-7.0 Ta; 6.0-6.4 Al; 1 to 1.5 Re; 0.6 to 0.7 Hf; 0.03 to 1.5 C; 0.004 to 0.015 B; if present, up to 0.03 total of a rare earth selected from Y, La, and Ce, and mixtures thereof; the balance being nickel and incidental impurities; wherein the superalloy composition exhibits creep rupture strength properties of at least 275 hours at a temperature of about 1600° F. (871° C.) and a cyclic load of about 70 ksi (483 MPa); wherein the superalloy composition exhibits creep rupture

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

PatentTitleYearCitations
US 11,739,398 B2Nickel-based superalloy20230

References Cited — Backward Prior Art (27)

PatentTitleYearCitations
JP S60141842 ANickel base superalloy—6
JP S60141843 ANickel base superalloy—6
US 4,719,080 AAdvanced high strength single crystal superalloy compositions1988209
US 5,035,958 ANickel-base superalloys especially useful as compatible protective environmental coatings for advanced superaloys199149
US 5,043,138 AYttrium and yttrium-silicon bearing nickel-base superalloys especially useful as compatible coatings for advanced superalloys199140
JP H058263 AAutomatically mold replacing method in molding machine—7
US 5,240,518 ASingle crystal, environmentally-resistant gas turbine shroud199342
US 5,399,313 ANickel-based superalloys for producing single crystal articles having improved tolerance to low angle grain boundaries1995111
US 5,435,861 ANickel-based monocrystalline superalloy with improved oxidation resistance and method of production199549
US 5,451,142 ATurbine engine blade having a zone of fine grains of a high strength composition at the blade root surface199553
JP H0841566 AOxidation resistant nickel-base single crystal alloy and its production—6
JP H09157777 ANickel base alloy excellent in thermal fatigue resistance, high temperature creep resistance and high temperature corrosion resistance—21
US 5,660,649 AMethod of making oxidation resistant single crystal superalloy castings199716
JP H10168534 ATurbine blade and its production—6
US 6,007,645 AAdvanced high strength, highly oxidation resistant single crystal superalloy compositions having low chromium content199973
US 6,074,602 AProperty-balanced nickel-base superalloys for producing single crystal articles200094
US 6,096,141 ANickel-based superalloys exhibiting minimal grain defects200016
EP 1,038,983 A1Single crystal nickel-base alloy—14
EP 1,184,473 A2Nickel-base single-crystal superalloys, method of manufacturing same and gas turbine high temperature parts made thereof—25
EP 1,201,778 A2Low density oxidation resistant superalloy materials capable of thermal barrier coating retention without a bond coat—31
US 6,521,053 B1In-situ formation of a protective coating on a substrate200316
US 6,673,308 B2Nickel-base single-crystal superalloys, method of manufacturing same and gas turbine high temperature parts made thereof200428
JP 2004285472 ANickel superalloy for manufacturing single crystal member—2
US 2004229072 A1Nickel base superalloy—26
JP 2005097649 ANi-BASED SUPERALLOY—23
US 6,966,956 B2Ni-based single crystal super alloy200528
US 2007163682 A1Ni-based superalloy having high oxidation resistance and gas turbine part—7

Non-Patent Literature (5)

  • English Abstract and English Machine Translation of Harada et al. (JP 2005-097649)(2005).
  • Office Action from corresponding JP Application No. 2010523067, dated Jun. 25, 2013.
  • Office Action from corresponding JP Application No. 2010523068, dated Jun. 25, 2013.
  • PCT International Search Report and Written Opinion issued Feb. 12, 2009 in connection with corresponding Application No. PCT/US2008/074171.
  • PCT International Search Report and Written Opinion issued Feb. 18, 2009 in connection with corresponding Application No. PCT/US2008/074168.