Polyacrylic acid (salt)-type water absorbent resin and method for producing of same
Abstract
A process for producing a water absorbent resin is provided with which it is possible to efficiently and inexpensively obtain a surface-crosslinked water-absorbing resin having excellent material properties, while ensuring high productivity. In continuous production scaled up to a large scale (in particular, 1 t/hr or more), the physical properties are improved and stabilized (for example, a reduction in standard deviation of the physical properties) by a surface crosslinking treatment to further improve absorption against pressure (AAP) and saline flow conductivity (SFC). The process for producing a polyacrylic acid (salt)-type water absorbent resin includes a surface treatment step in which after addition of a surface-crosslinking agent, a crosslinking reaction is conducted in a transverse type continuous stirring apparatus having stirring means including a feeding inlet and a discharging outlet of a water absorbent resin and one or more rotary shafts having with a plurality of stirring discs, and heating means, at a stirring-power index of the device of 3-15 W·hr/kg. (Stirring-power index)=((power consumption of apparatus at the time surface treatment)−(power consumption at the
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method for producing a polyacrylic acid (salt)-type water absorbent resin, comprising a step of preparing an aqueous monomer solution of an acrylic acid (salt), a step of continuously polymerizing the aqueous monomer solution, a step of finely shredding a hydrous gel-like crosslinked polymer during or after polymerization, a step of drying the obtained particulate hydrous gel-like crosslinked polymer, and a surface treatment step of adding and reacting a surface treatment agent to and with the dried water absorbent resin powder, wherein crosslinking reaction is carried out at a stirring powe
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (50)
Non-Patent Literature (5)
- Chinese Office Action dated Feb. 14, 2014 in CN 201080038386.5, and English translation thereof.
- Chinese Office Action, dated Aug. 29, 2013, in related CN Appln. No. 201080038386.5, and its English translation.
- Chinese Office Action, dated Jan. 15, 2013, in corresponding CN Appln. No. 201080038386.5, and its English translation.
- Chinese Office Action, dated Jan. 15, 2013, in related CN Appln. No. 201080038364.9, and its English translation.
- Chinese Office Action, dated Sep. 17, 2013, in related CN Appln. No. 201080038364.9, and its English translation.