Patents
US 8,858,717 B2#7820961 Most CitedActiveUnited States (USPTO)Utility

Inhibiting corrosion and scaling of surfaces contacted by sulfur-containing materials

13Forward Citations (#7820961 Global)
1.1/yrCitation Velocity (#5959086 Global)
1.83Citation PageRank (#16727974 Global)
46Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

A method of treatment for inhibiting sulfur-based corrosion or scaling or for removing scaling from a surface including inhibiting corrosion caused by sulfur-containing materials, reducing corrosion caused by sulfur-containing materials, inhibiting scaling caused by sulfur-containing and sulfur-containing materials in gas, liquid or solid phase or any combination of multiple phases of materials, reducing scaling caused by sulfur-containing and sulfur-containing materials, and removing scaling caused by sulfur-containing and sulfur-containing materials. The method involves contacting sulfur-containing materials with a composition containing a turpentine liquid. The method also involves contacting corrodible surfaces or surfaces prone to scaling with a composition containing a turpentine liquid.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 46 · Forward citations: 13.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of treatment for inhibiting sulfur-based corrosion or scaling or for removing scaling from a surface in contact with or prone to contact with sulfur-containing material, said method selected from the group consisting of inhibiting corrosion caused by sulfur-containing materials, reducing corrosion caused by sulfur-containing materials, inhibiting scaling caused by sulfur-containing materials, reducing scaling caused by sulfur-containing materials, and removing scaling caused by sulfur-containing materials, comprising contacting said sulfur-containing material with a substantially non-

  2. Claim 2Depends on #1

    The method of claim 1 , wherein said t

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • "Sulfur," Kirk-Othmer Encyclopedia of Chemical Technology, vol. 23, 5th Edition, pp. 1-37, Nov. 2006.
  • Bates.: "Elemental Sulfur as a Corrodent in Deaerated, Neutral Aqueous Solutions," Materials Performance, p. 56, 1981.
  • Chertkov et al.: "Corrosion activity of hydrocarbon fuels in the presence of elemental sulfur," Khimiia i tekhnologiia topliv i masel, vol. 3, No. 7, pp. 62-66, 1958.
  • Chow et al.: "Fluor SOx cleanup process a cost effective "SO2 to elemental sulfur" technology for global green environment," 2006 TMS Fall Extraction and Processing Division: Sohn International Symposium, vol. 8, Abstract, 1 page, 2006.
  • Cobb et al.: "Methods of Operation to Prevent Sulfite Liquor Evaporator Fouling," Pulping Conference, Proceedings of the Technical Association of the Pulp and Paper Industry, Abstract, p. 459, 1984.