Patents
US 8,852,811 B2#18923527 Most CitedActiveUnited States (USPTO)Utility

Process for producing lithium manganate particles and non-aqueous electrolyte secondary battery

6Forward Citations (#18923527 Global)
0.5/yrCitation Velocity (#16163999 Global)
1.16Citation PageRank (#33992523 Global)
13Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

According to the present invention, there is provided a process for producing lithium manganate particles having a high output and an excellent high-temperature stability. The present invention relates to a process for producing lithium manganate particles comprising the steps of mixing a lithium compound, a manganese compound and a boron compound with each other; and calcining the resulting mixture in a temperature range of 800 to 1050° C., wherein an average particle diameter (D 50 ) of the boron compound is not more than 15 times an average particle diameter (D 50 ) of the manganese compound, and wherein the lithium manganate particles have a composition represented by the following chemical formula: Li 1+x Mn 2-x-y Y1 y O 4 +B in which Y1 is at least one element selected from the group consisting of Ni, Co, Mg, Fe, Al, Cr and Ti, and x and y satisfy the conditions of 0.03≦x≦0.15 and 0≦y≦0.20, respectively.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 6.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A process for producing lithium manganate particles comprising the steps in this order of: mixing a lithium compound, a manganese compound and a boron compound with each other; and calcining the resulting mixture in a temperature range of 800 to 1050° C., in which an average particle diameter (D 50 ) of the boron compound is not more than 15 times an average particle diameter (D 50 ) of the manganese compound.

  2. Claim 2Depends on #1

    A process for producing lithium manganate particles according to claim 1 , wherein the average particle diameter (D 50 ) of the boron compound is 1 μm to 100 μm.

  3. Claim 3Depends on #1

    A process for producing lithium manganate particles according to claim 1 , wherein the average particle diameter (D 50 ) of the manganese compound is 1 μm to 20 μm.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (3)

  • International Preliminary Report on Patentability (English version) in PCT/JP2009/004636 dated Apr. 28, 2011.
  • International Search Report for PCT/JP2009/004636, mailed Oct. 27, 2009.
  • Supplementary European Search Report dated Jun. 28, 2013 of corresponding European Patent Application No. 09814294.6-1355 / 2330079, PCT/JP2009004636 (7 pgs).