Patents
US 8,840,817 B2#133770534 Most CitedActiveUnited States (USPTO)Utility

Preparation method for asphalt-based spherical activated carbon which requires no infusibilization process

0Forward Citations (#133770534 Global)
0.0/yrCitation Velocity (#133770534 Global)
0.56Citation PageRank (#133770534 Global)
7Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The present invention is a preparation method for asphalt-based spherical activated carbon which requires no infusibilization process. Placing coal tar asphalt into a melting device; introducing compressed air of 0.1 MPa-0.5 MPa into the device and stirring until a melting temperature of 280° C.-350° C. is reached; continuing for 2-8 hours until the base material has a softening point of 200° C.-260° C.; after cooling down, pulverizing the base material to obtain asphalt powder. Obtaining 34%-79% by mass of carbon powder, 1%-10% by mass of binder, and 20%-65% by mass of the asphalt powder and then forming spherical particles with a diameter of 0.5 mm-5 mm with the carbon powder, the binder and the asphalt powder at room temperature. Introducing the spherical particles of asphalt directly into an asphalt carbonization furnace for carbonization at a temperature of 600° C.-900° C. under protection of an inert gas to obtain asphalt spherical carbon. Asphalt spherical carbon is subject to activation treatment to obtain asphalt spherical activated carbon. The preparation method of the present invention reduces processing difficulty and production costs significantly.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A preparation method for asphalt-based spherical activated carbon which requires no infusibilization process, characterized in that it is specifically carried out in accordance with the following steps: Step 1: Preparing asphalt powder Selecting coal tar asphalt as a base material and placing it into a melting device; introducing compressed air of 0.1 MPa-0.5 MPa into the device and stirring the base material until a melting temperature of 280° C.-350° C. is reached; continuing for 2-8 hours until the base material has a softening point of 200° C.-260° C.; after cooling down, pulverizing the b

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.