Patents
US 8,835,309 B2#99801200 Most CitedActiveUnited States (USPTO)Utility

Forming nickel—platinum alloy self-aligned silicide contacts

0Forward Citations (#99801200 Global)
0.0/yrCitation Velocity (#99801200 Global)
0.56Citation PageRank (#99801200 Global)
13Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A method of performing a silicide contact process comprises a forming a nickel-platinum alloy (NiPt) layer over a semiconductor device structure; performing a first rapid thermal anneal (RTA) so as to react portions of the NiPt layer in contact with semiconductor regions of the semiconductor device structure, thereby forming metal rich silicide regions; performing a first wet etch to remove at least a nickel constituent of unreacted portions of the NiPt layer; performing a second wet etch using a dilute Aqua Regia treatment comprising nitric acid (HNO 3 ), hydrochloric acid (HCl) and water (H 2 O) to remove any residual platinum material from the unreacted portions of the NiPt layer; and following the dilute Aqua Regia treatment, performing a second RTA to form final silicide contact regions from the metal rich silicide regions.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of performing a silicide contact process, the method comprising: forming a nickel-platinum alloy (NiPt) layer over a semiconductor device structure; performing a first rapid thermal anneal (RTA) so as to react portions of the NiPt layer in contact with semiconductor regions of the semiconductor device structure, thereby forming metal rich silicide regions; performing a first wet etch to remove at least a nickel constituent of unreacted portions of the NiPt layer, the first wet etch comprising a standard clean (SC-1) etch using ammonium hydroxide (NH 4 OH) and hydrogen peroxide (H 2 O

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (2)

  • E. Alptekin et al., "Tuning of the Platinum Silicide Schottky Barrier Height on n-Type Silicon by Sulfur Segregation," IEEE Electron Device Letters, vol. 30, No. 4, Apr. 2009, pp. 331-333.
  • F. Goh et al., "Challenges in Nickel Platinum Silicide Wet Etching for Sub-65nm Device Technology," ECS Trans., vol. 11, No. 2, 2007, pp. 321-326.