Patents
US 8,823,015 B2#9655007 Most CitedActiveUnited States (USPTO)Utility

Silicon carbide epitaxial wafer and manufacturing method therefor

11Forward Citations (#9655007 Global)
0.9/yrCitation Velocity (#7811440 Global)
1.65Citation PageRank (#19752660 Global)
9Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Provided is a silicon carbide epitaxial wafer, the entire surface of which is free of step bunching. Also provided is a method for manufacturing said silicon carbide epitaxial wafer. The provided method for manufacturing a silicon carbide semiconductor device includes: a step wherein a 4H—SiC single-crystal substrate having an off-axis angle of 5° or less is polished until the lattice disorder layer on the surface of the substrate is 3 nm or less; a step wherein, in a hydrogen atmosphere, the polished substrate is brought to a temperature between 1400° C. and 1600° C. and the surface of the substrate is cleaned; a step wherein silicon carbide is epitaxially grown on the surface of the cleaned substrate as the amounts of SiH 4 gas and C 3 H 8 gas considered necessary for epitaxially growing silicon carbide are supplied simultaneously at a carbon-to-silicon concentration ratio between 0.7 and 1.2 to 1; and a step wherein the supply of SiH 4 gas and the supply of C 3 H 8 gas are cut off simultaneously, the substrate temperature is maintained until the SiH 4 gas and the C 3 H 8 gas are evacuated, and then the temperature is decreased.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 11.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A SiC epitaxial wafer obtained by forming a SiC epitaxial layer on a 4H—SiC single-crystal substrate that is tilted at an off-angle of 0.4° to 5°, wherein when a surface of the SiC epitaxial wafer layer is measured by an optical surface inspection device that uses laser light, mean-square roughness Rq of the surface is 1.3 nm or less, and wherein linear density of steps of the epitaxial layer surface of the wafer is 5 mm −1 or less.

  2. Claim 2Depends on #1

    The SiC epitaxial wafer according to claim 1 , wherein the steps are connected to shallow pits due to screw dislocation in the SiC epitaxial layer.

  3. Claim 3Independent Claim

    A SiC epitaxial wafer obtained by forming a SiC epitaxial layer on a 4H—SiC single-crystal substrate that is tilted at an off-angle of 0.4° to 5°, wherein when a surface of the SiC epitaxial wafer layer is measured by an ato

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • Christian Hecht et al., "Thick epitaxial layers on 4° off-oriented 4H-SiC suited for PiN-diodes with blocking voltages above 6.5 kV", Materials Science Forum, 2006, pp. 239-242, vols. 527-529, Trans Tech Publications, Switzerland.
  • International Search Report for PCT/JP2010/064375 dated Oct. 5, 2010.
  • Keiji Wada et al., "Epitaxial growth of 4H-SiC on 4° off-axis (0001) and (0001) substrates by hot-wall chemical vapor deposition", Journal of Crystal Growth 291, 2006, pp. 370-374, Elsevier.
  • M. Treu et al., "Challenges and First Results of SiC Schottky Diode Manufacturing using a 3 inch Technology", Materials on Science Forum, 2004, pp. 981-984, vols. 457-460, Trans Tech Publications, Switzerland.