Patents
US 8,815,059 B2#22449175 Most CitedActiveUnited States (USPTO)Utility

System and/or method for heat treating conductive coatings using wavelength-tuned infrared radiation

5Forward Citations (#22449175 Global)
0.4/yrCitation Velocity (#19428589 Global)
1.11Citation PageRank (#36256973 Global)
40Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Certain example embodiments relate to systems and/or methods for preferentially and selectively heat treating conductive coatings such as ITO using specifically tuned near infrared-short wave infrared (NIR-SWIR) radiation. In certain example embodiments, the coating is preferentially heated, thereby improving its properties while at the underlying substrate is kept at low temperatures. Such techniques are advantageous for applications on glass and/or other substrates, e.g., where elevated substrate temperatures can lead to stress changes that adversely effect downstream processing (such as, for example, cutting, grinding, etc.) and may sometimes even result in substrate breakage or deformation. Selective heating of the coating may in certain example embodiments be obtained by using IR emitters with peak outputs over spectral wavelengths where the conductive coating (or the conductive layer(s) in the conductive coating) is significantly absorbing but where the substrate has reduced or minimal absorption.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 40 · Forward citations: 5.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of making a coated article, the method comprising: providing a glass substrate; forming a layer comprising indium tin oxide on the substrate via physical vapor deposition, wherein the layer comprising indium tin oxide is located between and directly contacting a first layer comprising silicon nitride and a second layer comprising silicon nitride; exposing the glass substrate with the layer comprising indium tin oxide thereon to near infrared radiation at a peak emission of 1-2 μm for up to about 108 seconds so as to cause the sheet resistance, emissivity, and absorption to be lower th

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (40)

PatentTitleYearCitations
GB 2,031,756 ANon-iridescent glass structures and processes for their production—66
US 5,093,207 ALaminate material or laminate workpiece with a functional layer, especially a friction bearing layer, disposed on a backing layer199239
US 5,344,718 AHigh performance, durable, low-E glass1994279
EP 0,634,376 A1Process for treating a thin oxide layer—17
EP 0,646,660 A1Production of carriers for surface plasmon resonance—18
JP H07114841 ATransparent conductive film and its forming and working method—47
WO 9,513,189 A1Abrasion wear resistant coated substrate product—47
EP 0,676,379 A2Production technique for a glass plate coated with a semi-reflective silver layer—26
US 5,514,476 ALow-E glass coating system and insulating glass units made therefrom1996291
EP 0,719,876 A2Annealed low emissivity coating—30
US 5,557,462 ADual silver layer Low-E glass coating system and insulating glass units made therefrom1996287
US 5,584,902 AMethod of converting coated glass1996197
US 5,770,321 ANeutral, high visible, durable low-e glass coating system and insulating glass units made therefrom1998216
US 5,800,933 ANeutral, high performance, durable low-E glass coating system and insulating glass units made therefrom1998301
US 6,042,752 ATransparent conductive film, sputtering target and transparent conductive film-bonded substrate200090
US 6,059,909 ANeutral, high visible, durable low-E glass coating system, insulating glass units made therefrom, and methods of making same200075
US 2001041252 A1Low-emissivity glass coatings having a layer of nitrided nichrome and methods of making same—49
US 2002031674 A1Low-emissivity glass coatings having a layer of silicon oxynitride and methods of making same—69
US 2002071903 A1Method for preparing transparent conductive thin film by rapid thermal annealing method—20
US 2003142705 A1High energy, high average power solid state green or UV laser—9
US 6,635,321 B2Vacuum IG window unit with edge seal formed via microwave curing, and corresponding method of making the same200360
US 6,641,689 B1Vacuum IG window unit with peripheral seal at least partially diffused at temper200388
US 6,686,050 B2Heat treatable low-E coated articles and methods of making same2004207
US 6,701,749 B2Vacuum IG window unit with edge seal at least partially diffused at temper and completed via microwave curing, and corresponding method of making the same2004103
US 2004147139 A1Rapid energy transfer annealing device and process—35

Non-Patent Literature (5)

  • "A Full Description of a Simple and Scalable Fabrication Process for Electrowetting Displays", Zhou et al., Journal of Micromechanics and Microengineering 19, (2009) pp. 1-12.
  • "Homogeneously Aligned Liquid Crystal Display on Silicon Oxynitride Thin Film Using Ion Beam Bombardment"; Oh et al., Materials Chemistry and Physics 117 (2009) pp. 355-358.
  • U.S. Appl. No. 12/457,006, Broadway et al., filed May 28, 2010.
  • U.S. Appl. No. 12/659,196, Lemmer et al., filed Feb. 26, 2010.
  • U.S. Appl. No. 12/662,894, Lemmer et al., filed May 10, 2010.