Patents
US 8,809,170 B2#9207020 Most CitedActiveUnited States (USPTO)Utility

High throughput cyclical epitaxial deposition and etch process

11Forward Citations (#9207020 Global)
0.9/yrCitation Velocity (#7770463 Global)
2.42Citation PageRank (#10684742 Global)
50Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Methods of selective formation leave high quality epitaxial material using a repeated deposition and selective etch process. During the deposition process, an inert carrier gas is provided with a silicon-containing source without hydrogen carrier gas. After depositing silicon-containing material, an inert carrier gas is provided with an etchant to selectively etch deposited material without hydrogen. The deposition and etch processes can be repeated until a desired thickness of silicon-containing material is achieved. Using the processes described within, it is possible to maintain temperature and pressure conditions, as well as inert carrier gas flow rates, to provide for increased throughput. The inert flow can be constant, or etch rates can be increased by reducing inert flow for the etch phases of the cycles.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 11.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for selectively forming silicon-containing material over single crystal semiconductor surfaces, comprising: providing a substrate, the substrate comprising insulating surfaces and single-crystal semiconductor surfaces; depositing silicon-containing material over the insulating surfaces and single crystal semiconductor surfaces of the substrate by flowing a silicon-containing source vapor and an inert carrier gas without flowing H 2 ; selectively removing silicon-containing material from over the insulating surfaces by flowing an etchant while maintaining continuous flow of the inert c

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 4,058,430 AMethod for producing compound thin films19771,251
US 4,210,925 AI2 L Integrated circuit and process of fabrication198025
US 4,413,022 AMethod for performing growth of compound thin films1983555
US 4,521,952 AMethod of making integrated circuits using metal silicide contacts198581
US 4,578,142 AMethod for growing monocrystalline silicon through mask layer1986101
US 4,605,947 ATitanium nitride MOS device gate electrode and method of producing198670
US 4,698,316 AMethod of depositing uniformly thick selective epitaxial silicon198742
US 4,704,186 ARecessed oxide method for making a silicon-on-insulator substrate198724
US 4,710,241 AMethod of making a bipolar semiconductor device198736
US 4,728,623 AFabrication method for forming a self-aligned contact window and connection in an epitaxial layer and device structures employing the method198880
US 4,735,918 AVertical channel field effect transistor198818
US 4,747,367 AMethod and apparatus for producing a constant flow, constant pressure chemical vapor deposition1988274
US 4,749,441 ASemiconductor mushroom structure fabrication198843
US 4,749,440 AGaseous process and apparatus for removing films from substrates1988629
US 4,758,531 AMethod of making defect free silicon islands using SEG198899
US 4,761,269 AApparatus for depositing material on a substrate1988366
US 4,778,775 ABuried interconnect for silicon on insulator structure198830
US 4,786,615 AMethod for improved surface planarity in selective epitaxial silicon198864
US 4,793,872 AIII-V Compound heteroepitaxial 3-D semiconductor structures utilizing superlattices198850