Method for producing alkali metal niobate particles, and alkali metal niobate particles

0Forward Citations (#96520992 Global)
0.0/yrCitation Velocity (#96520992 Global)
0.56Citation PageRank (#96520992 Global)
7Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Disclosed are a method of producing fine particulate alkali metal niobate in a liquid phase system, wherein the size and shape of the particulate alkali metal niobate can be controlled; and fine particulate alkali metal niobate having a controlled shape and size. One of specifically disclosed is a method of producing a substantially rectangular cuboid particulate alkali metal niobate represented by MNbO 3 (1), wherein M represents one element selected from alkaline metals, including specific four steps. Another one of specifically disclosed is particulate alkali metal niobate represented by the formula (1) having a substantially rectangular cuboid shape, wherein the substantially rectangular cuboid shape has a longest side and a shortest side, the length of the longest side represented by an index L max is 0.10 to 25 μm, and the length of the shortest side represented by an index L min is 0.050 to 15 μm.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 0.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method of producing particulate alkali metal niobate represented by the following formula (1): MNbO 3   (1) wherein M represents one element selected from alkaline metals, the particulate alkali metal niobate having a substantially rectangular cuboid shape, the method comprising the steps of: (a) mixing a niobium-containing solution with an alkaline solution having a concentration of 0.1 to 30 mol/L, to prepare a suspension; (b) allowing the suspension to stand still for 12 to 48 hours at a temperature between 80° C. and 150° C.; (c) performing a solvothermal reaction of the suspension at a

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein M in the formula (1) is N

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (4)

  • Amini and Mirzaee, Effect of solvent and temperature on the preparation of potassium niobate by hydrothermal-assisted sol-gel processing, Ceramics International, 35 (2009) 2367-2372.
  • Saito, et al., "Synthesis of polycrystalline platelike KNbO3 particles by the topochemical micro-crystal conversion method and fabrication of grain-oriented (K0.5Na0.5)NbO3 ceramics", Journal of the European Ceramic Society 27, 2007, pp. 4085-4092.
  • Sun, et al., "Hydrothermal Synthesis of Single Crystalline (K, Na)NbO3 Powders", Eur. J. Inorg. Chem., 2007, pp. 1884-1888.
  • Wang, et al., "Hydrothermal synthesis of potassium niobate powders", Ceramics International, 2007, vol. 33, No. 7, pp. 1611-1615.