Baseball with improved core and enhanced durability
Abstract
A baseball capable of being tested under ASTM F1887-09 wherein the baseball is projected at a strike plate at a speed of approximately 60 mph to measure the COR of the baseball. The baseball includes a core formed of a diene-based rubber composition, at least one layer of yarn surrounding the core, and a cover assembly surrounding the one layer of yarn. The core has a diameter of less than 2.0 inches and a weight less than 1.5 ounces. The baseball has a circumference of less than 9.5 inches and a weight of less than 5.5 ounces. The baseball has an initial COR value when tested in accordance with ASTM F1887-09 and a second COR value measured after the baseball has undergone at least 60 impacts of approximately 60 mph against the strike plate. The second COR value is greater than 95 percent of the initial COR value.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 22 · Forward citations: 7.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A baseball capable of being tested under ASTM Standard Test Method F1888-09 for compression-displacement and under ASTM Standard Test Method F1887-09 wherein the baseball is projected at a strike plate at a speed of approximately 60 mph to measure the coefficient of restitution (COR) of the baseball, the baseball comprising: a core formed of a diene-based rubber composition, the core having a diameter of less than 2.0 inches and a weight less than 1.5 ounces; at least one layer of yarn surrounding the core; and a cover assembly surrounding the at least one layer of yarn, the baseball having a
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗