Patents
US 8,765,632 B2#38982377 Most CitedActiveUnited States (USPTO)Utility

Process for preparing catalyst comprising palladium supported on carrier with high dispersion

2Forward Citations (#38982377 Global)
0.2/yrCitation Velocity (#36545881 Global)
1.04Citation PageRank (#39418637 Global)
11Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

A process for preparing a catalyst comprising palladium supported on a carrier via a layered precursor, comprising the following steps: (1) synthesis of hydrotalcite layered precursor which comprises promoting metal element and aluminium on the surface of the carrier of A1 2 O 3 microspheres, the atoms of the promoting metal and aluminium being highly dispersed by each other and bonded firmly to the carrier due to the crystal lattice positioning effect of the hydrotalcite crystal; (2) introduction of palladium into the carrier through impregnation; (3) drying; and (4) calcination and reduction with H 2 , the hydrotalcite layered precursor being converted into a composite oxide which consists of oxides of the promoting metal and aluminium, and the promoting metal element and aluminium being highly dispersed by each other and being able to separate and disperse the mainly active palladium element loaded later. The process has the advantages of improving the catalytic performance of the catalyst, enhancing the stability of the catalyst, and achieving the object of reducing the consumption of the precious metal-palladium.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for preparing a supported catalyst containing palladium on a carrier, the process comprising: (1) preparing M 2+ Al-LDHs/Al 2 O 3 precursors, including: dissolving an amount of urea into deionized water to obtain a urea solution having a concentration of the urea in the range of 0.2 to 2 mol/L; adding Al 2 O 3 carriers having a mesh size of 26 to 100 with a regular geometry into the urea solution to obtain a second solution, where the content of the Al 2 O 3 carriers is 1 to 6 g/100 mL; stirring the second solution at 80 to 150° C. for 3 to 15 hours to obtain a mixed solution; pre

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)

Non-Patent Literature (3)

  • International Search Report issued in International Application No. PCT/CN2009/072453, mailed Oct. 1, 2009, 6 pages.
  • Takehira, et al., "Mechanism of reconstitution of hydrotalcite leading to eggshell-type Ni loading on Mg-Al mixed oxide", Journal of Catalysis, vol. 231, No. 1, Apr. 2005, pp. 92-104-Abstract only.
  • Takehira, et al., "Mechanism of reconstitution of hydrotalcite leading to eggshell-type Ni loading on Mg-Al mixed oxide", Journal of Catalysis, vol. 231, No. 1, Apr. 2005, pp. 92-104—Abstract only.