Patents
US 8,765,601 B2#21426509 Most CitedActiveUnited States (USPTO)Utility

Post deposition treatments for CVD cobalt films

5Forward Citations (#21426509 Global)
0.4/yrCitation Velocity (#19372242 Global)
1.39Citation PageRank (#25810438 Global)
18Prior Art Cited
3Claims (2 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Embodiments of the invention provide methods for forming materials on a substrate used for metal gate and other applications. In one embodiment, a method includes forming a cobalt stack over a barrier layer disposed on a substrate by depositing a cobalt layer during a deposition process, exposing the cobalt layer to a plasma to form a plasma-treated cobalt layer during a plasma process, and repeating the cobalt deposition process and the plasma process to form the cobalt stack containing a plurality of plasma-treated cobalt layers. The method further includes exposing the cobalt stack to an oxygen source gas to form a cobalt oxide layer from an upper portion of the cobalt stack during a surface oxidation process and heating the remaining portion of the cobalt stack to a temperature within a range from about 300° C. to about 500° C. to form a crystalline cobalt film during a thermal annealing crystallization process.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 18 · Forward citations: 5.

Claims (3 — 2 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for depositing materials on a substrate surface, comprising: forming a cobalt stack over a barrier layer disposed on a substrate by: depositing a cobalt layer during a deposition process; exposing the cobalt layer to a plasma to form a plasma-treated cobalt layer during a plasma process; and repeating the deposition process and the plasma process to form the cobalt stack, the cobalt stack comprising a plurality of plasma-treated cobalt layers; and heating the cobalt stack to a crystallization temperature within a range from about 300° C. to about 500° C. to form a crystalline cobalt f

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the cobalt stack comprises a carbon concentration of about 3 at% or less.

  3. Claim 3Independent Claim

    The method of

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗