Abstract

An APIX100-grade high strength steel pipe includes a base material containing, in mass percentage, C: more than 0.03% and 0.08% or less, Si: 0.01% to 0.5%, Mn: 1.5% to 3.0%, P: 0.015% or less, S: 0.005% or less, Al: 0.01% to 0.08%, Nb: 0.005% to 0.025%, Ti: 0.005% to 0.025%, N: 0.001% to 0.010%, O: 0.005% or less, and B: 0.0003% to 0.0020%, further contains one or more of Cu, Ni, Cr, Mo, and V, satisfies 0.19≦P cm ≦0.25, the balance being Fe and unavoidable impurities, and has a TS of 760 to 930 MPa, a uniform elongation of 5% or more, and a YR of 85% or less; the seam weld metal has a specific composition.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A high strength steel pipe for low-temperature usage comprising: a base material portion in which a base material has a composition containing, in mass percentage, C: more than 0.03% and 0.08% or less, Si: 0.01% to 0.5%, Mn: 1.5% to 3.0%, P: 0.015% or less, S: 0.003% or less, Al: 0.01% to 0.08%, Nb: 0.005% to 0.025%, Ti: 0.005% to 0.025%, N: 0.001% to 0.010%, O: 0.005% or less, and B: 0.0003% to 0.0020% and one or more of Cu: 0.01% to 1%, Ni: 0.01% to 1%, Cr: 0.01% to 1%, Mo: 0.01% to 1%, and V: 0.01% to 0.1%, wherein a P CM value (in %) calculated by a formula (1) below satisfies 0.19≦P CM ≦

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (15)

PatentTitleYearCitations
JP 2003293078 ASteel pipe having excellent weld heat affected zone toughness and deformability and method of producing steel sheet for steel pipe—10
JP 2003306749 AMethod for manufacturing high strength steel tube of excellent deformability and steel plate for steel tube—13
JP 2004131799 AHigh strength steel pipe excellent in deformability, low-temperature toughness and haz toughness, and its manufacturing method—30
JP 2006233263 AMethod for producing high strength welded steel tube having excellent low yield ratio and weld zone toughness—18
JP 2006265577 AMethod for producing high strength, high toughness steel sheet—26
JP 2006328523 AHigh strength steel pipe for low temperature use—9
US 2007205001 A1Expandable Tubular—37
US 2007269335 A1Low alloy steel and weld joint thereof excellent in corrosion resistance to hydrochloric acid and sulfuric acid—9
JP 2008056961 AHIGH STRENGTH WELDED STEEL PIPE HAVING TENSILE STRENGTH OF 760 MPa OR MORE AND HAVING EXCELLENT TOUGHNESS IN WELDING HEAT-AFFECTED ZONE, AND MANUFACTURING METHOD THEREFOR—5
US 2008247900 A1Component for Machine Structure, Method of Producing the Same and Material for Induction Hardening—20
JP 2008248328 ALow yield ratio, high strength and high toughness steel sheet, and method for producing the same—25
JP 2008248330 ALow yield ratio high strength high toughness steel pipe and manufacturing method therefor—22
EP 2,006,407 A1High-strength steel plate with superior crack arrestability—21
JP 2009001909 AManufacturing method of high-strength cold-rolled steel sheet—11
US 2009025835 A1High Strength Steel Plate and High Strength Welded Pipe Excellent in Ductile Fracture Characteristic and Methods of Production of Same—21

Non-Patent Literature (1)

  • "Microstructure and Toughness of Weld Heat Affected Zone in Quenched-Tempered High Strength Steels", Journal of the Japan Welding Society, No. 50 (1981), a copy of partial English translation of Chapter 1 Introduction.