A wet friction member contains a pulverized cork heated to 150-200° C. if necessary. The pulverized cork is mixed with other papermaking materials and formed into a paper-made substrate. The paper-made substrate is impregnated with a synthetic resin to be a binder and heated and cured. The cork itself has a high friction coefficient μ. Moreover, a powder thereof increases surface area and area in contact with a separator plate of a counter member, thereby improving a friction coefficient of a friction surface of the wet friction member. The friction coefficient of the cork itself and capacities for absorbing and discharging oil are improved by heating the cork. Thus, there is provided a wet friction member that has a higher friction coefficient μ. An increase in the friction coefficient μ, weight reduction by reducing the number of friction members, and high efficiency are achieved when used as a wet friction member.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A wet friction member, comprising: a paper-made substrate made from base fibers and a pulverized cork mixed with the base fibers, and a synthetic resin as a binder impregnated and heated to be hardened in the paper-made substrate, wherein the pulverized cork comprises a heated pulverized cork that was subjected to a heat treatment for improving a discharge capacity of an oil film between a surface of the wet friction member and a separator plate as a counter member.

  2. Claim 2Depends on #1

    A wet friction member according to claim 1 , in which the pulverized cork has a median diameter within a range of 3 μm to 200 μm.

  3. Claim 3Depends on #1

    A wet friction member according to claim 1 , in which the heated pulverized cork was heated at a heating temperature within a range of 140° C. to 200° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.