Patents
US 8,765,107 B2#10818114 Most CitedActiveUnited States (USPTO)Utility

Process for straightening keratin fibres with a heating means and denaturing agents

10Forward Citations (#10818114 Global)
0.8/yrCitation Velocity (#8785539 Global)
1.59Citation PageRank (#20817016 Global)
5Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

The invention relates to a process for straightening keratin fibers, comprising: (i) a step in which a straightening composition containing at least two denaturing agents is applied to the keratin fibers, (ii) a step in which the temperature of the keratin fibers is raised, using a heating means, to a temperature of between 110 and 250° C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 5 · Forward citations: 10.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A process for relaxing keratin fibres, comprising: (i) applying to the keratin fibres a hair-relaxing composition containing at least two denaturing agents chosen from: (a) ureas of formula (I): in which R1, R2, R3 and R4 are independently chosen from: a hydrogen atom, and linear or branched C1-C4 lower alkyl or alkenyl radicals, optionally substituted with a radical chosen from hydroxyl, amino, and dimethylamino radicals, and (b) α-hydroxy acid derivatives of formula (IV): in which: R is chosen from OH and NR3R4, wherein R3 and R4 are independently chosen from hydrogen and linear or branched

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (2)

  • English translation of Japanese Office Action for Japanese Application No. 2009-511549, dated Mar. 15, 2012(4 pages).
  • Patent Abstracts of Japan for JP Publication No. 2003-212737 in English (1 page).