Patents
US 8,765,040 B2#35437978 Most CitedActiveUnited States (USPTO)Utility

Medical device fabrication process including strain induced crystallization with enhanced crystallization

2Forward Citations (#35437978 Global)
0.2/yrCitation Velocity (#36245575 Global)
1.33Citation PageRank (#27685205 Global)
34Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Methods of fabricating a polymeric implantable device, such as a stent, with improved fracture toughness through annealing a polymer construct below the glass transition temperature of the polymer of the construct prior to a deformation step are disclosed herein. The deformation of the construct induces crystallization in the polymer construct through strain-induced crystallization. The annealing of the polymer construct accelerates the crystallization induced during the deformation and results in an increase in crystallite density with smaller crystallites as compared to deformation of a tube that has not been annealed. A stent scaffolding is then made from the deformed tube.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 34 · Forward citations: 2.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method of making a stent comprising: annealing an extruded PLLA tube at a temperature range of 40 to 50° C., wherein the PLLA tube is annealed for a selected annealing time greater than 1 min, wherein the annealing increases the nucleation density of the PLLA tube; cooling the PLLA tube to below 30° C. at the end of the selected annealing time; followed by heating and radially expanding the PLLA tube, wherein the cooling of the PLLA tube to below 30° C. is prior to the heating and the radially expanding, wherein the radial expansion induces crystallization in the PLLA tube, wherein the incre

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (34)

PatentTitleYearCitations
US 5,211,902 AMethod of reducing residual stresses in thermoplastic laminates199317
US 5,650,485 ANon-oxidizing polymeric medical implant199797
US 6,319,576 B1Method to increase the crystallization rate of polyesters200135
US 2003069629 A1Bioresorbable medical devices—92
US 2003083732 A1Balloon expandable polymer stent with reduced elastic recoil—118
US 2004181271 A1Intraluminal prostheses having polymeric material with selectively modified crystallinity and methods of making same—52
US 6,932,930 B2Intraluminal prostheses having polymeric material with selectively modified crystallinity and methods of making same2005102
US 2006246108 A1Amorphous poly(D,L-lactide) coating—54
US 2007032634 A1Method for extending shelf-life of constructs of semi-crystallizable polymers—9
US 2007038290 A1Fiber reinforced composite stents—97
US 2007135898 A1Polymeric stent having modified molecular structures in the flexible connectors and the radial arcs of the hoops—3
US 2007132156 A1Polymeric stent having modified molecular structures in selected regions of the hoops and method for making the same—16
US 2007200271 A1Implantable device prepared from melt processing—22
US 2007253999 A1Method of fabricating an implantable medical device to reduce chance of late inflammatory response—34
US 2007253996 A1Method of fabricating an implantable medical device by controlling crystalline structure—18
US 7,297,758 B2Method for extending shelf-life of constructs of semi-crystallizable polymers20076
US 2007283552 A1Manufacturing process for polymeric stents—99
WO 2007/142736 A2Manufacturing process for polymeric stents—32
EP 1,872,808 A1Polymeric stent having modified molecular structures in selected regions of the hoops and method for increasing elongation at break—15
US 2008014240 A1Stereocomplex-forming composition and implantable medical device comprising same—20
WO 2008/008495 A2Stereocomplex-forming composition and implantable medical device comprising same—11
US 2008051873 A1Bioabsorbable polymeric medical device—40
US 2008169582 A1Method and apparatus for making polymeric drug delivery devices having differing morphological structures—14
US 2008177374 A1Biodegradable endoprostheses and methods for their fabrication—29
US 2009248147 A1Stent With Nucleating Agent—15
US 2010025894 A1Tube expansion process for semicrystalline polymers to maximize fracture toughness—49
US 2010036478 A1Method Of Improving Fracture Toughness Of Implantable Medical Devices Through Annealing—32
WO 2010/017090 A2Tube expansion process for semicrystalline polymers to maximize fracture toughness—17

Non-Patent Literature (5)

  • Anderson et al., "Melt preparation and nucleation efficiency of polylactide stereocomplex crystallites", Polymer 47, pp. 2030-2035 (2006).
  • Borokhovskii et al., "Thermodynamic analysis of nucleus formation in crystallization of polymers", Vysokomol. Soyed. A18, No. 11, pp. 2406-2411 (1976).
  • Brizzolara et al., "Mechanism of the Stereocomplex Formation between Enantiomeric Poly(lactide)s", Macromolecules, vol. 29, pp. 191-197 (1996).
  • Brostow, "Performance of Plastics", Hanser Gardner Publ. 1st Ed. pp. 254-255 (2000).
  • International Search Report for PCT/US2009/053029, mailed Aug. 12, 2010, 8 pgs.