Method for producing high-purity tungsten powder

3Forward Citations (#33935779 Global)
0.2/yrCitation Velocity (#29088595 Global)
0.98Citation PageRank (#42841955 Global)
13Prior Art Cited
2Claims (1 Indep. · 1 Dep.)
0Drawings / Sheets

Abstract

Provided is a method for producing a high-purity tungsten powder having a phosphorus content of less than 1 wtppm; wherein an ammonium tungstate solution containing 1 wtppm or more of phosphorus as an impurity in terms of the inclusion in tungsten is used as a starting material, this solution is neutralized with hydrochloric acid at a temperature of 50° C. or less to adjust the pH at 4 or more and less than 7 so as to precipitate ammonium paratungstate undecahydrate crystals, the resulting solution is heated to 70 to 90° C. and filtered in a high-temperature state so as to obtain ammonium paratungstate pentahydrate crystals, the obtained crystals are calcined so as to form a tungsten oxide, and the tungsten oxide is subject to hydrogen reduction so as to obtain a high-purity tungsten powder. Additionally provided is a method for producing a high-purity tungsten powder having a phosphorus content of 0.4 wtppm or less; wherein the ammonium tungstate solution is neutralized with hydrochloric acid to adjust the pH at 4 or more and 6 or less, and this solution is subject to the same procedure as described above so as to obtain a high-purity tungsten powder. Consequently, the phosphorus

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 13 · Forward citations: 3.

Claims (2 — 1 Independent, 1 Dependent)

  1. Claim 1Independent Claim

    A method for producing a high-purity tungsten powder having a phosphorus content of less than 1 wtppm; wherein an ammonium tungstate solution is used as a starting material and neutralized with hydrochloric acid at a temperature of 50° C. or less to adjust the pH at 4 or more and less than 7 so as to precipitate ammonium paratungstate undecahydrate crystals, the resulting solution is heated to 70 to 90° C. and filtered while at a temperature of 70 to 90° C. so as to obtain ammonium paratungstate pentahydrate crystals, the obtained crystals are calcined so as to form a tungsten oxide, and the t

  2. Claim 2Depends on #1

    The method according to claim 1 , wherein the ammonium tungstate solution used as the starting material has a content of phosphorus of 1 wt